A technology of conductive grease and silver powder, which is used in cable/conductor manufacturing, circuits, conductive materials dispersed in non-conductive inorganic materials, etc. problems, to achieve the effect of low oil diffusion and evaporation loss, simple process, and reduced contact wear
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] 1) Weigh synthetic base oil, pure copper powder, tin powder, and silver powder. The mass percentages of the synthetic base oil, pure copper powder, tin powder, and silver powder are 60% of synthetic base oil, 33% of pure copper powder, and 1% of tin powder. %, silver powder 1%;
[0020] 2) Add synthetic base oil, pure copper powder, tin powder, and silver powder into the reactor and mix evenly to obtain a paste mixture for later use;
[0021] 3) Weighing the lithium soap, crushing the lithium soap to obtain lithium soap powder, the mass percentage of the lithium soap is 5%;
[0022] 4) Add lithium soap powder to the paste mixture, mix well, stir and grind to obtain conductive grease;
[0023] 5) Put the conductive grease into the packaging bottle to get the finished product.
Embodiment 2
[0025] 1) Weigh synthetic base oil, pure copper powder, tin powder, and silver powder. The mass percentages of the synthetic base oil, pure copper powder, tin powder, and silver powder are 63% of synthetic base oil, 23% of pure copper powder, and 2% of tin powder. %, silver powder 2%;
[0026] 2) Add synthetic base oil, pure copper powder, tin powder, and silver powder into the reactor and mix evenly to obtain a paste mixture for later use;
[0027] 3) Weighing the lithium soap, crushing the lithium soap to obtain lithium soap powder, the mass percentage of the lithium soap is 10%;
[0028] 4) Add lithium soap powder to the paste mixture, mix well, stir and grind to obtain conductive grease;
[0029] 5) Put the conductive grease into the packaging bottle to get the finished product.
Embodiment 3
[0031] 1) Weigh synthetic base oil, pure copper powder, tin powder, and silver powder. The mass percentages of the synthetic base oil, pure copper powder, tin powder, and silver powder are 60% of synthetic base oil, 23% of pure copper powder, and 1% of tin powder. %, silver powder 1%;
[0032] 2) Add synthetic base oil, pure copper powder, tin powder, and silver powder into the reactor and mix evenly to obtain a paste mixture for later use;
[0033] 3) Weighing the lithium soap, crushing the lithium soap to obtain lithium soap powder, the mass percentage of the lithium soap is 15%;
[0034] 4) Add lithium soap powder to the paste mixture, mix well, stir and grind to obtain conductive grease;
[0035] 5) Put the conductive grease into the packaging bottle to get the finished product.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com