A slow-release technology for pests and diseases, applied in fertilization devices, fertilizer mixtures, applications, etc., can solve the problems of no way to reduce the processing cost of superabsorbent resin, the imbalance of trace element ratio, and hinder the application and promotion of superabsorbent resin, etc. Achieve the effects of avoiding soil erosion, good water retention performance, and improving water use efficiency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0026] 1) Put 50 parts by weight of acrylic acid in a container, add 350 parts by weight of deionized water and stir evenly, adjust the pH value with potassium hydroxide, and make the system pH value around 7.0;
[0027] 2) Weigh 30 parts by weight of dry natural sheep dung and crush it into 100 mesh powder;
[0028] 3) Add the sheep dung powder prepared in step 2) to the solution prepared in step 1, then add 60 parts by weight of urea, 10-15 parts by weight of diammonium phosphate, stir to dissolve, and stir at high speed for 30 minutes with nitrogen;
[0029] 4) Heat the solution of step 3 to 65°C for 20 minutes under a pressure of 0.03 Mpa;
[0030] 5) Add 1.0 part by weight of potassium persulfate, add 1.0 part by weight of sodium sulfite, and after stirring uniformly, add 0.5 part by weight of crosslinking agent N,N'-methylene bispresentenamide, and polymerize at a temperature of 50°C. The time is 1 hour to obtain a cross-linked polymer product;
[0031] 6) Transfer the cross-link...
Embodiment 2
[0035] 1) Put 80 parts by weight of acrylic acid in a container, add 350 parts by weight of deionized water and stir evenly, adjust the pH value with potassium hydroxide to make the system pH around 7.0;
[0036] 2) Weigh 50 parts by weight of dry natural sheep dung and crush it into 100 mesh powder;
[0037] 3) Add the sheep dung powder prepared in step 2) to the solution prepared in step 1, then add 90 parts by weight of urea, 15 parts by weight of diammonium phosphate, stir and dissolve, and stir at high speed with nitrogen for 30 minutes;
[0038] 4) Heat the solution of step 3 to 65°C for 20 minutes under a pressure of 0.05 Mpa;
[0039] 5) Add 1.0 part by weight of oxidant potassium persulfate, 1.0 part by weight of reducing agent sodium sulfite, and after stirring uniformly, add 0.5 part by weight of cross-linking agent N,N'-methylene bispresentenamide, at a temperature of 60°C Polymerize, and the polymerization time is 1 hour to obtain a cross-linked polymerization product;
[...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com