Functional admixture used for early tensioning prestressed structural concrete and purposes of functional admixture
A prestressed structure and admixture technology, which is applied in sustainable waste treatment, solid waste management, climate sustainability, etc., can solve the problems of long construction period and long prestressed age, and achieve high elastic modulus in the early stage. , The effect of improving the early elastic modulus and reducing the turnover cycle of the template
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0024] Carbonate stone powder preparation: Calcite is crushed and ground into carbonate stone powder.
[0025] The proportion of functional admixture is: carbonate stone powder: 70%; fly ash: 10%; ground slag powder: 20%.
[0026] Concrete mix ratio (kg / m 3 ): Cement: 384; Functional admixture: 96; Fine aggregate: 750; Coarse aggregate: 1080; Water: 129; Water reducing agent: 4.8.
[0027] Concrete properties: initial slump 220mm, air content 2.4%, 1d compressive strength 34.9MPa, 3d compressive strength 50.8MPa, 28d compressive strength 59.1MPa, 1d elastic modulus 27.1GPa, 3d elastic modulus 37.5GPa, the Concrete is used for the construction of cast-in-place beams, and the tension requirements can be met in 3d.
Embodiment 2
[0029] Carbonate stone powder preparation: Dolomite is crushed and ground into carbonate stone powder.
[0030] The proportion of functional admixtures is: carbonate stone powder: 95%; ground slag powder: 5%.
[0031] Concrete mix ratio (kg / m 3 ): Cement: 376; Functional admixture: 75; Fine aggregate: 760; Coarse aggregate: 1050; Water: 152; Water reducing agent: 1.9.
[0032] Concrete properties: initial slump 200mm, air content 3.1%, 3d compressive strength 53.6MPa, 5d compressive strength 64.5MPa, 28d compressive strength 74.8MPa, 3d elastic modulus 40.5GPa, 28d elastic modulus 47.2GPa, the Concrete is used for the construction of cast-in-place beams, and the tension requirements can be met in 3d.
Embodiment 3
[0034] Carbonate stone powder preparation: the tailings and stone chips in the limestone mining process are crushed and ground into carbonate stone powder.
[0035] The proportion of functional admixtures is: carbonate stone powder: 40%, silica fume 20%, fly ash: 40%;
[0036] Concrete mix ratio (kg / m 3 ): Cement: 488; Functional admixture: 166; Fine aggregate: 601; Coarse aggregate: 1116, Water: 195.2, Water reducing agent: 5.6;
[0037] Concrete properties: initial slump is 180mm, air content is 3.8%, 3d compressive strength 42.2MPa, 28d compressive strength 57.2MPa, 3d elastic modulus 42.3GPa, this concrete is used for cast-in-place beam construction, 3d can satisfy tension Claim.
PUM
Property | Measurement | Unit |
---|---|---|
length | aaaaa | aaaaa |
compressive strength | aaaaa | aaaaa |
compressive strength | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com