Embodiment 1
[0024] Present embodiment comprises following weight components:
[0025] Hydroxypropyl cellulose 500g;
[0026] Polyvinyl alcohol 70g;
[0027] Povidone K30 100g;
[0028] Polyethylene glycol 6000 120g;
[0029] Glyceryl triacetate 50g;
[0031] 600g of water;
[0032] Carmine 1g;
[0033] Carmine lake 30g;
[0034] Titanium dioxide 50g.
[0035] Mix the above amounts of hydroxypropyl cellulose, polyvinyl alcohol, povidone K30, polyethylene glycol 6000, titanium dioxide, glycerol triacetate, talcum powder, and water for 1 hour, dry at 40°C for 5 hours, and take the intermediate for detection , after passing the test, add carmine lake according to the above amount, mix for 0.5 hours, transfer to a grinder and grind for 5 hours, sieve, take the intermediate for testing, add the above amount of carmine to adjust, and mix for 1 hour. After the semi-finished product passes the inspection, pack , made of red film coating.
Embodiment 2
[0037] Present embodiment comprises following weight components:
[0038] Polyacrylic resin II 600g;
[0039] Polyvinyl alcohol 60g;
[0040] Povidone K30 80g;
[0041] Polyethylene glycol 6000 100g;
[0042] Glyceryl triacetate 10g;
[0044] 400g of water;
[0045] Lemon yellow 50g;
[0046] Lemon Yellow Aluminum Lake 10g;
[0047] Titanium dioxide 150g.
[0048] The preparation method of this embodiment is the same as that of Example 1.
Embodiment 3
[0050] Present embodiment comprises following weight components:
[0051] Microcrystalline cellulose 300g;
[0052] Methylcellulose 400g;
[0053] Polyvinyl alcohol 50g;
[0054] Povidone K30 120g;
[0055] Polyethylene glycol 6000 80g;
[0056] Glyceryl triacetate 100g;
[0057] Talc powder 90g;
[0058] 500g of water;
[0059] Bright blue 20g;
[0060] Brilliant blue aluminum lake 100g;
[0061] Titanium dioxide 100g.
[0062] The preparation method of this embodiment is the same as that of Example 1.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology