Embodiment 1
[0012] The concrete additive that present embodiment provides comprises the following components by weight:
[0013] Methacrylic acid 100 Sodium hydroxide 33
[0014] Hydroxyethyl cellulose 0.0 4 Potassium persulfate 0.04
[0015] Polyethylene glycol acrylate 0.01
[0016] The preparation method of the concrete additive provided in this embodiment is to add 100 kilograms of methacrylic acid into a reaction vessel with a stirrer, then add a sodium hydroxide solution with a solid content of 33 kilograms for neutralization, and the degree of neutralization is 60%. Then add 0.04 kg of hydroxyethyl cellulose, 0.04 kg of potassium persulfate and 0.01 kg of polyethylene glycol acrylate to the neutralizing solution in turn, react for 60-80 minutes, and finally mix with concrete and send to the construction site.
Embodiment 2
[0018] The concrete additive that present embodiment provides comprises the following components by weight:
[0019] Methacrylic acid 100 Sodium hydroxide 50
[0020] Hydroxyethylcellulose 0.06 Potassium persulfate 0.06
[0021] Polyethylene glycol acrylate 0.03
[0022] The preparation method of the concrete additive provided in this embodiment is to add 100 kilograms of methacrylic acid into a reaction vessel with a stirrer, then add a sodium hydroxide solution with a solid content of 50 kilograms for neutralization, and the degree of neutralization is 90%. Then add 0.06 kg of hydroxyethyl cellulose, 0.06 kg of potassium persulfate and 0.03 kg of polyethylene glycol acrylate to the neutralizing solution in turn, react for 60-80 minutes, and finally mix it with concrete and send it to the construction site.
Embodiment 3
[0024] Methacrylic acid 100 Sodium hydroxide 41
[0025] Hydroxyethylcellulose 0.05 Potassium persulfate 0.05
[0026] Polyethylene glycol acrylate 0.02
[0027] The preparation method of the concrete additive provided in this embodiment is to add 100 kilograms of methacrylic acid into a reaction vessel with a stirrer, then add a sodium hydroxide solution with a solid content of 41 kilograms for neutralization, and the degree of neutralization is 60%. Then add 0.05 kg of hydroxyethyl cellulose, 0.05 kg of potassium persulfate and 0.02 kg of polyethylene glycol acrylate to the neutralizing solution in sequence, react for 60-80 minutes, and finally mix with concrete and send to the construction site.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com