Embodiment 1
[0009] Using a single-screw sheet extruder, the surface of the roller of the sheet extruder is set with multiple identical patterns or groups of identical characters. These identical patterns or characters have a certain distance from each other. These identical patterns Or the text is raised or lowered. Using such a sheet extruder unit, polymer materials with shape memory properties, such as norbornene, trans polyisoprene, polyurethane, styrene-butadiene copolymer, polyethylene, etc., are exchanged with peroxide. Cross-linking process or one-step silane cross-linking process, cross-linking in the barrel of the extruder, and extruding into a sheet with concave-convex patterns or characters on the surface corresponding to the roller, the thickness of the sheet is 0.1-2mm, and the thickness of the sheet is 0.3- 0.5mm is better. Then heat the above-mentioned cross-linked sheet, then use a two-roll or three-roll calender to flatten the concave-convex pattern or characters on the ...
Embodiment 2
[0011] Polymer materials with shape memory function, such as norbornene, trans-polyisoprene, polyurethane, styrene-butadiene copolymer, ethylene-vinyl acetate polymer, polyethylene, etc., are cross-linked with peroxide Process or one-step silane crosslinking process, crosslink these materials in the barrel of the injection molding machine, and then use the mold to directly form concave-convex patterns (text) on the surface of the injection molded product. When the injection molded product is heated above its deformation temperature, the pattern (text) formed on its surface is pressed into other patterns (text), or pressed into a plane, and then these products are heated above its deformation temperature. Injection molding The formed concave-convex pattern (character) will reappear.
Embodiment 3
[0013] Use peroxide cross-linking process or one-step silane cross-linking process to cross-link polymer materials with shape memory function such as norbornene, trans polyisoprene, polyurethane, styrene-butadiene copolymer , ethylene-vinyl acetate polymer, polyethylene and other polymer materials with shape memory functions are extruded into flat sheets, and the sheets are cut into the required specifications according to the size of the hot-pressing mold, and then the sheets are put into the hot-pressing mold In the process, a concave-convex pattern (character) is hot-pressed on the surface of the sheet. The thickness of the sheet with concavo-convex patterns (characters) is 0.1-2.0mm. The thickness of the planar sheet is 0.1-2.0 mm. When it is necessary to check the authenticity of the product, put the small pieces into boiling water or heat them in other ways, and these small pieces will return to flat sheets, which will play the role of anti-counterfeiting.
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com