A plastering mortar and deodorizing technology, applied in the field of plastering mortar materials, can solve the problems of secondary pollution of the air environment, reduced farm productivity, reduced disease resistance, etc., and achieves the effects of low manufacturing cost, prevention of cross-infection, and simple production process.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0031] Put 35Kg of cement, 45Kg of construction sand, 2Kg of superfine alumina, 5Kg of sepiolite nanofiber, 3Kg of copper oxide superfine powder, and 20Kg of water into the concrete mixer to mix the ingredients, then add 10Kg of rare earth activated antibacterial agent, and stir thoroughly for 5 Minutes, mix well and use directly.
[0032] The mortar material is used in building construction, and it has good antibacterial and deodorizing functions. After testing, the plastering mortar material with antibacterial, deodorant and anti-algae materials can significantly reduce the concentration of odorous substances such as ammonia in animal farms, and realize animal health. healthy farming. The inorganic antibacterial and deodorant material in the mortar material has long-term antibacterial function, which can kill the bacteria adsorbed on the surface and avoid cross infection between bacteria, thereby effectively reducing the production of odorous substances such as ammonia gas; ...
Embodiment 2
[0034] Put 45Kg of cement, 40Kg of construction sand, 2Kg of superfine silica, 3Kg of polymer fiber, 2Kg of superfine zinc oxide powder, and 25Kg of water into the concrete mixer to mix the ingredients, then add 8Kg of zeolite antibacterial agent, stir for 5 minutes, and mix Use directly after smoothing.
[0035] Its technical effect is the same as embodiment 1.
Embodiment 3
[0037] Put 40Kg of cement, 37Kg of construction sand, 2Kg of superfine magnesium oxide powder, 3Kg of sepiolite nanofiber, 3Kg of superfine magnesium oxide powder, and 17Kg of water into the concrete mixer to mix the ingredients, then add 15Kg of phosphate antibacterial agent, fully Stir for 5 minutes, mix well and use directly.
[0038] Its technical effect is the same as embodiment 1.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com