Novel technique for extracting aluminum oxide from coal gangue
A technology of coal gangue and new process is applied in the field of comprehensive utilization of coal gangue, which can solve the problems of complex process, no chemical reactivity and high energy consumption, and achieve the effects of saving aluminum ore resources, reducing environmental pollution and ecological destruction of vegetation.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0006] Example 1: First, coal gangue is processed according to the following procedure: 50 g of coal gangue is crushed and ground to a particle size of less than 0.074 μm, and roasted at 660° C. for 0.5 hour. At 98°C, take hydrochloric acid with a concentration of 15% and add a certain amount of coal gangue to prepare a solid-liquid ratio of 1:4 (ratio of the mass of coal gangue to the mass of hydrochloric acid) (g / g), and the speed of the electric mixer is 340r / min, react for 80 minutes, cool to room temperature, and then use a centrifuge to separate the solid from the liquid, put the separated solid in an oven, heat it to 95°C, and dry it for 4 hours. After drying, pure Al can be obtained 2 o 3 .
Embodiment 2
[0007] Example 2: Firstly, coal gangue is processed according to the following procedure: 50 g of coal gangue is crushed and ground to a particle size of less than 0.074 μm, and roasted at 680° C. for 45 minutes. At 98°C, take hydrochloric acid with a concentration of 20% and add a certain amount of coal gangue to prepare a solid-liquid ratio of 1:5 (ratio of the mass of coal gangue to the mass of hydrochloric acid) (g / g), and the speed of the electric mixer is 360r / min, react for 90 minutes, cool to room temperature, and then use a centrifuge to separate the solid from the liquid, put the separated solid in an oven, heat it to 100°C, and dry it for 5 hours. After drying, pure Al can be obtained 2 o 3 .
Embodiment 3
[0008] Example 3: Firstly, coal gangue is processed according to the following procedure: 50 g of coal gangue is crushed and ground until the particle size is less than 0.074 μm, and roasted at 750° C. for 55 minutes. At 98°C, take hydrochloric acid with a concentration of 30% and add a certain amount of coal gangue to prepare a solid-liquid ratio of 1:6 (ratio of the mass of coal gangue to the mass of hydrochloric acid) (g / g), and the speed of the electric mixer is 370r / min, react for 100 minutes, cool to room temperature, and then use a centrifuge to separate the solid from the liquid, put the separated solid in an oven, heat it to 100°C, and dry it for 6 hours. After drying, pure Al can be obtained 2 o 3 .
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com