A heterogeneous oxidation, diphenyl carbonate technology, applied in the preparation of carbon dioxide or inorganic carbonate, metal/metal oxide/metal hydroxide catalyst, physical/chemical process catalyst, etc., can solve the difficulty of catalyst recovery, problems such as low selectivity and yield, to achieve the effect of simple and convenient preparation process, simple preparation and lower production cost
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0026] Preparation of Mn-Cu double metal oxides by co-precipitation method: take 4.1g MnSO 4 ·H 2 O, add 15ml of deionized water to dissolve and prepare a solution; another 0.9g CuSO 4 , add 15ml of deionized water to make a solution; mix the two solutions, add 4ml of 20% sodium carbonate aqueous solution for precipitation, and keep stirring, filter after aging for 24 hours, and then dry the precipitate in vacuum Drying in an oven at 100°C for 12 hours; then roasting the dried material in a muffle furnace at 600°C for 7 hours to obtain a manganese-based composite oxide carrier;
[0027] Take PdCl 2 Dissolve 40mg in 40ml of deionized water, adjust the pH value of the solution to about 1 with concentrated hydrochloric acid, and heat to dissolve; add the manganese composite oxide carrier prepared above into the solution, and adjust the pH value to 8 with NaOH solution to precipitate The active component was stirred continuously for 2 hours, then filtered, dried, and finally c...
Embodiment 2
[0030] Mn-Ce bimetallic oxides were prepared by indirect mechanical grinding method, taking 4.2 g MnSO 4 ·H 2 0, add 15ml deionized water to dissolve, be mixed with solution; Add 4ml concentration and be 20% sodium carbonate aqueous solution and carry out precipitation, and aging 10 hours, filter, obtain manganese carbonate precursor; Then manganese carbonate precursor is in vacuum oven Dry for 12 hours; then bake the dried product in a muffle furnace at 600°C for 7 hours to obtain manganese oxide; take another 0.8g CeO 2 , mix and stir the two oxides on a grinder evenly, dry the mixture in a vacuum oven at 100°C for 12 hours; then bake the dried product in a muffle furnace at 500°C for 8 hours to obtain a manganese-based oxide catalyst support;
[0031] Take PdCl 2 Dissolve 40 mg in 40 ml of deionized water, adjust the pH value of the solution to about 1 with concentrated hydrochloric acid, then heat to dissolve, add the above-mentioned manganese composite oxide catalyst c...
Embodiment 3
[0034] Mn-Pb double metal oxides were prepared by direct mechanical milling method, taking 3.2 g MnCO 3 , another 1.8g PbCO 3 , mix and stir the two salts on a grinder evenly, dry the mixture in a vacuum oven at 100°C for 12 hours; Catalyst carrier;
[0035] Take PdCl 2 Dissolve 40 mg in 40 ml of deionized water, drop the pH value of the solution to about 1 with concentrated hydrochloric acid, then heat and dissolve, add the manganese composite oxide catalyst carrier prepared above into the solution, and then add NaOH alkali solution to adjust the pH value to 9, to precipitate active components, and kept stirring for 3 hours, then filtered, dried, and finally roasted at 200°C for 3 hours to obtain the final catalyst, with a palladium loading of 0.5%;
[0036] Get 1.0g above-mentioned prepared catalyst, 47g phenol, 1g tetrabutylammonium bromide, 74mg benzoquinone respectively and join in the autoclave of 250ml, pass into O 2 The pressure of CO is 0.3MPa, the pressure of CO...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com