Thermal barrier coating and preparation method thereof

A thermal barrier coating, nickel-based superalloy technology, applied in coatings, devices for coating liquids on surfaces, layered products, etc., can solve problems such as cracking, sliding, peeling off thermal barrier coatings, etc. The effect of cracking, stress relaxation, shear resistance enhancement

Inactive Publication Date: 2009-11-25
严格集团股份有限公司
View PDF2 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0003] The purpose of the present invention is to solve the problems in the prior art that the material interface in the direction parallel to the nickel-based superalloy layer is relatively sliding and falling off and the thermal barrier coating is vertically cracked in the direction perpendicular to the nickel-based superalloy layer. Provide a kind of preparation method of thermal barrier coating

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Thermal barrier coating and preparation method thereof
  • Thermal barrier coating and preparation method thereof
  • Thermal barrier coating and preparation method thereof

Examples

Experimental program
Comparison scheme
Effect test

specific Embodiment approach 1

[0008] Embodiment 1: The thermal barrier coating in this embodiment is composed of an outer ceramic layer 1 and an inner bonding layer 5, wherein the inner bonding layer 5 is composed of a nickel-based superalloy layer 4 and a bonding layer connected to the outer surface of the nickel-based superalloy layer 4. The bonding layer 2 is composed of nickel three-dimensional structure 3 and yttria-stabilized zirconia; wherein the nickel three-dimensional structure 3 is a honeycomb nickel space structure.

specific Embodiment approach 2

[0009] Embodiment 2: This embodiment differs from Embodiment 1 in that the nickel three-dimensional structure 3 in the adhesive layer 2 is connected to the outer surface of the nickel-based superalloy 4 through electrodeposition. Others are the same as in the first embodiment.

specific Embodiment approach 3

[0010] Embodiment 3: This embodiment is different from Embodiment 1 in that the thickness of the adhesive layer (2) is 30-60 μm. Others are the same as in the first embodiment.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

PropertyMeasurementUnit
thicknessaaaaaaaaaa
thicknessaaaaaaaaaa
Login to view more

Abstract

A method for preparing a thermal barrier coating relates to a method for preparing a coating. It solves the problems in the prior art that the material interface in the direction parallel to the nickel-based superalloy layer is relatively sliding and falling off and the thermal barrier coating is vertically cracked in the direction perpendicular to the nickel-based superalloy layer in the prior art. The thermal barrier coating is composed of an outer ceramic layer (1) and an inner bonding layer (5), wherein the inner bonding layer (5) is composed of a nickel-based superalloy layer (4) and the outer surface of the nickel-based superalloy layer (4) The bonding layer (2) is composed of a nickel three-dimensional structure (3) and yttria-stabilized zirconia; wherein the nickel three-dimensional structure is a honeycomb nickel spatial structure. Preparation method: Electrodeposit on the outer surface of the nickel-based superalloy layer (4) to obtain a three-dimensional nickel structure connected to it, then spray yttrium oxide-stabilized zirconia sol, calcinate to obtain the bonding layer (2), and then coat the bonding layer (2) Prepare the ceramic layer (1) on it to obtain a thermal barrier coating.

Description

technical field [0001] The invention relates to a method for preparing a coating. Background technique [0002] Thermal barrier coatings have been widely used in many fields such as aviation, aerospace, gas power generation, metallurgy, shipbuilding, chemical industry and automobile manufacturing. The development of science and technology has put forward higher and higher requirements on the working temperature and service life of the hot end components. Therefore, it is necessary to vigorously develop thermal barrier coatings with high performance, high reliability and long life. Traditional thermal barrier coatings are usually composed of a ceramic surface layer and a bonded bottom layer. The thermal barrier coating structure can be mainly divided into two-layer structure, multi-layer structure and gradient structure. Due to the complexity and diversity of thermal barrier coating conditions, thermal barrier coatings often lead to failure. The failure of existing thermal...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Patents(China)
IPC IPC(8): B32B33/00B32B7/10C25D5/40C25D5/24C25D5/50C25D3/12B05D5/00C23D3/00
Inventor 马彬李垚
Owner 严格集团股份有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products