Carbonate deposition method of crystal type heavy rare earth
A carbonate precipitation and heavy rare earth technology, applied in the direction of improving process efficiency, can solve the problems of affecting rare earth recovery rate, high product moisture content, high precipitation cost, convenient transportation and subsequent use, high rare earth recovery rate, The effect of low moisture content in the product
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0007] 1200L heavy rare earth chloride solution after mixed rare earth extraction and grouping, rare earth concentration 1.47M, acidity 0.78N, main impurity Fe 2 o 3 183mg / L, CaO 30.5mg / L, PbO 0.8mg / L, rare earth distribution Dy 2 o 3 0.11%, Ho 2 o 3 2.075%, Er 2 o 3 7.99%, Tm 2 o 3 0.99%, Yb 2 o 3 5.7%, Lu 2 o 3 0.77%, Y 2 o 3 81.8%, the calculated average molecular weight is 122.13, and the heavy rare earth chloride solution contains 215.44Kg of heavy rare earth oxides. Add the heavy rare earth chloride solution to the precipitation tank first, adjust the pH value of the heavy rare earth chloride solution to 5.2 with 10% ammonium bicarbonate water under stirring, add 3.6L polyacrylamide saturated aqueous solution and fully stir and mix, let it stand for clarification for 5 hours; The above solution is filtered, the filtrate is pumped to the sedimentation tank with a pump, diluted with water to 0.5M, and 251.33Kg of heavy rare earth carbonate reserved fo...
Embodiment 2
[0010] After mixed rare earth extraction and grouping, heavy rare earth chloride solution 1500L, rare earth concentration 1.55M, acidity 0.66N, main impurity Fe 2 o 3 205mg / L, CaO 32.2mg / L, PbO 0.68mg / L, rare earth distribution Dy 2 o 3 0.08%, Ho 2 o 3 2.18%, Er 2 o 3 8.03%, Tm 2 o 3 0.94%, Yb 2 o 3 5.57%, Lu 2 o 3 0.69%, Y 2 o 3 82.06%, the calculated average molecular weight is 121.8, and the heavy rare earth chloride solution contains 283.19Kg of heavy rare earth oxides. Add the heavy rare earth chloride solution into the sedimentation tank, adjust the pH value of the heavy rare earth chloride solution to 5.0 with 8% ammonium bicarbonate water under stirring conditions, add 1.5L polyacrylamide saturated aqueous solution and fully stir and mix, let it stand for clarification for 2 hours, and The above solution is filtered, the filtrate is pumped to the sedimentation tank with a pump, diluted with water to 0.4M, and 242.24Kg of heavy rare earth carbonate...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com