Production of composite rubber track
A technology of compound rubber and manufacturing method, applied in household components, applications, household appliances, etc., can solve the problems of high tensile strength, poor sunlight crack resistance, environmental pollution, etc., and achieve good impact absorption performance and product return Good elasticity, the effect of non-toxic volatiles
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
example 1
[0014] Example 1, (1) First take by weight 20 parts of neoprene, 30 parts of natural rubber, 50 parts of EPDM, 20 parts of white carbon black, 40 parts of clay, 5 parts of zinc oxide, stearin 2 parts of acid, 8 parts of naphthenic oil, 8 parts of dizinc ester, 2 parts of antioxidant, 0.5 part of ultraviolet absorber, 2 parts of accelerator NS, 1.5 parts of accelerator ETU, 1.5 parts of sulfur, flame retardant chlorinated paraffin 15 parts, flame retardant decabromodiphenyl ether 30 parts, vulcanized rubber powder 50 parts.
[0015] (2) cutting raw rubber into small pieces;
[0016] (3) All materials are mixed in an internal mixer, the mixing temperature is 80-120°C, the mixing time is 10min, and the glue is removed at 120°C;
[0017] (4) Press the mixed rubber into tablets, apply a release agent and park for 12 hours;
[0018] (5) Put the parked rubber into the 18-inch open mill to add vulcanization and produce sheets for later use;
[0019] (6) Lay the fabric and the recla...
example 2
[0022] Example 2, (1) First take by weight 30 parts of neoprene, 25 parts of natural rubber, 45 parts of EPDM, 25 parts of white carbon black, 35 parts of clay, 5 parts of zinc oxide, stearin 1.5 parts of acid, 10 parts of naphthenic oil, 6 parts of dizinc ester, 2.5 parts of antioxidant, 0.8 part of ultraviolet absorber, 2.5 parts of accelerator NS, 2 parts of accelerator ETU, 1.6 parts of sulfur, flame retardant chlorinated paraffin 18 parts, flame retardant decabromodiphenyl ether 35 parts, vulcanized rubber powder 40 parts.
[0023] (2) cutting raw rubber into small pieces;
[0024] (3) All materials are mixed in an internal mixer, the mixing temperature is 80-120°C, the mixing time is 10min, and the glue is removed at 120°C;
[0025] (4) Press the mixed rubber into tablets, apply a release agent and park for 12 hours;
[0026] (5) Put the parked rubber into the 18-inch open mill to add vulcanization and produce sheets for later use;
[0027] (6) Lay the fabric and the ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com