Method of realizing clean combustion of petroleum coke
A coke cleaning and petroleum coke technology, which is applied in the field of clean utilization of petroleum coke, can solve problems such as insufficient reaction, poor sulfur removal effect, large calcium carbonate, etc., and achieves reduced use cost, complete and sufficient sulfur removal reaction, and high specific surface area increased effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0048] Take 5 kg of petroleum coke and firstly process it through high-pressure roller milling to crush the petroleum coke into a powder below 1-2 mm, then make the treated coarse powder into a slurry with a solid content of 68% with water, and then enter the ultra-fine cyclone The ultra-fine treatment in the mill becomes particles with an average particle size of less than 1 micron, and then put into the storage tank.
[0049] Take 1 kg of 200-mesh heavy calcium, adjust it into a slurry with a solid content of 65% with water, then enter it into an ultra-fine swirl mill for ultra-fine treatment, and then put it into a storage tank.
[0050] The petroleum coke slurry and the heavy calcium slurry are fully mixed in the swirl mill, burned through the combustion nozzle, and the SO in the flue gas is measured 2 The content is 92mg.
Embodiment 2
[0052] Take 5 kg of petroleum coke and first pass through high-pressure roller milling to crush the petroleum coke into a powder with a size of 1 to 2 mm, then add 1 kg of 200 mesh heavy calcium to the processed coarse powder, and adjust it with water to form a slurry with a solid content of 68%. shape, and then enter the ultra-fine swirl mill for ultra-fine treatment to become particles with an average particle size of less than 1 micron, and then put them into the storage tank. Combustion through combustion nozzles and measurement of SO in the flue gas 2 The content is 80mg.
Embodiment 3
[0054] Take 5 kg of petroleum coke and first pass through high-pressure roller milling to crush the petroleum coke into a powder with a size of 1 to 2 mm, then make the treated coarse powder into a slurry with a solid content of 50% with water, and add the chemical desulfurizer NaOH About 550 grams, then enter the ultra-fine swirl mill for ultra-fine treatment, and then put it into the storage tank.
[0055] The treated petroleum coke slurry is separated from solid and liquid by a centrifuge and washed three times with water. The separated and washed petroleum coke is then put into storage tanks.
[0056] The washed petroleum coke slurry is adjusted for solid content, burned through the combustion nozzle, and the SO in the flue gas is measured 2 The content is 2.1mg.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com