Carbon material electrical heating membrane and preparing method
An electric heating film and carbon material technology, applied in electric heating devices, ohmic resistance heating, heating element materials, etc., can solve the problems that electric heating films cannot be used on a large scale, low electrothermal conversion rate, unusable, etc. The electric effect is obvious, the preparation process is simple, and the effect of easy industrialization
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] Embodiment 1 of the present invention: 100 grams of emulsified chloroprene rubber is diluted with a special diluent provided by the merchant, and the addition of the diluent is 300 grams, which is used to adjust the viscosity of the slurry, while adding 3 grams of carbon black dispersant DP -983, after uniform dispersion, first add 40 grams of conductive carbon black to disperse for 0.8 hours, then add 61 grams of graphite carbon powder to disperse for 0.8 hours, put the dispersed slurry into a Raymond mill for 1 hour, and then put it into Disperse in the disperser for 0.8 hours. According to the characteristics of the coating machine, add 100 grams of diluent to adjust the viscosity of the slurry in each dispersion and grinding to make a coating slurry; use the coating machine to evenly prepare the prepared slurry Coating on glass fiber cloth and drying, the process parameter is to keep warm at 60°C for 25 minutes, the thickness of each coating is beneficial to prevent ...
Embodiment 2
[0018] Embodiment 2 of the present invention: Dilute 100 grams of high-temperature epoxy resin with epoxy resin diluent, the addition of diluent is 400 grams, for adjusting the viscosity of slurry, add 3 grams of carbon black dispersant DP-983 simultaneously After dispersing evenly, first add 60 grams of conductive carbon black to disperse for 0.5 hours, then add 36 grams of graphite carbon powder and 10 grams of stabilizer Al 2 o 3 Disperse for 0.5 hours, put the dispersed slurry into a sand mill and grind for 2 hours, and then put it into a disperser to disperse for 0.5 hours. According to the characteristics of the coating machine, add 50 grams of diluent to each dispersion and grinding to adjust The viscosity of the slurry is used to prepare the slurry for coating; the prepared slurry is evenly coated on the glass fiber cloth with a coating machine and dried. The process parameters are 120 ° C for 15 minutes, 160 ° C for 15 minutes, Keep warm at 200°C for 15 minutes. The ...
Embodiment 3
[0019] Embodiment 3 of the present invention: 100 grams of high-temperature phenolic resins are diluted with high-temperature phenolic resin diluents, and the addition amount of diluents is 200 grams, is used for adjusting the viscosity of slurry, adds 3 grams of carbon black dispersants DP-983 simultaneously, After uniform dispersion, first add 30 grams of conductive carbon black to disperse for 1 hour, then add 40 grams of graphite carbon powder and 20 grams of stabilizer SiO 2 Disperse for 1 hour, put the dispersed slurry into the three-roller and roll it continuously for 4 times, and then put it into the disperser to disperse for 1 hour. According to the characteristics of the coating machine, add dilution 150 grams of additives to adjust the viscosity of the slurry to prepare the slurry for coating; the prepared slurry is evenly coated on the glass fiber cloth with a coating machine and dried. The process parameters are 180 ° C for 25 minutes, each The thickness of the co...
PUM
Property | Measurement | Unit |
---|---|---|
service temperature | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com