Anticorrosive wear-resistant flexible ceramic powder coating
A flexible ceramic, anti-corrosion and wear-resistant technology, applied in the fields of flexible ceramic coatings, wear-resistant, anti-corrosion, can solve the problems of not meeting the needs of anti-corrosion, wear-resistant, impact resistance, hazards to construction personnel, high labor intensity, etc., to achieve good durability Impact performance, eliminate internal stress, improve the effect of temperature change resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0019] Component A of this coating is prepared according to the following ratio (mass ratio): first, mix the three epoxy resins in a ratio of 10:8:4, then take 20% of the above three epoxy resins mixed in proportion, and take 15% permeate, 9% titanium carbide, 10% wollastonite, 20% silicon powder, 5% superfine zinc oxide, 20% mixed solvent, 0.5% dispersing wetting agent, 0.5% leveling agent.
[0020] The preparation process is as follows: according to the above ratio, the film-forming material, filler and other raw materials are mixed in a mixing tank with a disperser and dispersed evenly, then pumped into the grinding equipment, ground to the required average particle size, and sieved. Package. And pack B component in another can according to the maximum amount of 1 / 10 of A component.
Embodiment 2
[0022] This coating is prepared according to the following component ratios (mass ratio), get 22% of epoxy resin mixed in the ratio of Example 1, 26% of silicon micropowder, 15% of wollastonite, 10% of titanium carbide, and 5% of flash stone %, dispersant 1%, wetting agent 1%, mixed solvent 20%.
[0023] The preparation method is the same as in Example 1.
Embodiment 3
[0025] The coating is prepared according to the following composition ratio (mass ratio): 20% mixed epoxy resin, 50% silica powder, 5% wollastonite, 3% titanium carbide, 4% flashstone, 1% dispersant, and Wet agent 2%, mixed solvent 20%.
[0026] The preparation method is the same as in Example 1.
[0027] The examples are only used to illustrate the technical solutions of the present invention, and are not intended to limit the present invention.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com