Method for synthesizing polypren phosphate
A technology of polypentenyl phosphate and synthesis method, applied in the direction of phosphorus organic compounds, etc., to achieve the effect of simple source
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0060] A kind of polypentenyl phosphate synthetic method, comprises the following steps:
[0061] In the first step, an oily substance with a plant polyprenol content higher than 85%, for example, a plant polyprenol content of 90%, is added to a non-polar organic solvent to form a mixed solution, and phosphorus is catalyzed by a nitrogen-containing organic base. Add the acylating agent dropwise to the above mixed solution, and stir at a speed of 50-800rpm while adding dropwise. The stirring speed can be selected as 100rpm, 350rpm, or 740rpm. °C, 25 °C, 36 °C, 48 °C, 55 °C, 62 °C, 74 °C, 79 °C, and make the reactant in a vacuum of 50-200 mmHg, for example, the vacuum can be selected as 100 mmHg, 160 mmHg After the dropwise addition, continue to react for 1 to 4 hours. For example, the reaction time can be selected as 1.2 hours, 2.5 hours, and 3.4 hours to obtain a mixed solution containing the reaction product.
[0062] Wherein, the structure of plant polyprenol is (H 3 c) 2...
Embodiment 2
[0067] Synthesis of Polypentenyl Phosphate Monoester Using Pyrophosphoric Acid as Phosphorylating Agent
[0068] Take 5 g of refined polyprenol samples, dissolve them in 70 ml of carbon tetrachloride solution, and transfer them to a 250 ml three-neck flask. Take 3.5g of pyrophosphoric acid solution, add it to 70ml of carbon tetrachloride solution, and then slowly drop it into the reactor for reaction, the dropping rate is 1-5ml / min., the reaction temperature is 50°C-60°C, and the stirring speed is 100-800r / min. Min, the vacuum degree is 50-200mmHg, after 2 hours of reaction, add 3 grams of triethylamine, continue the reaction for 1-2 hours, then add 80ml of acetone, 20ml of water and 0.5ml of triethylamine to carry out catalytic and hydrolysis reactions. The reaction temperature is 65°C-75°C, the stirring speed is 100-800r / min, the vacuum degree is 50-200mmHg, and the reaction time is 1-2 hours. Stop the reaction, add 100ml of water and 0.5ml of triethylamine after cooling, e...
Embodiment 3
[0070] Synthesis of Polypentenyl Dichlorophosphate Using Phosphorus Oxychloride as Phosphorylation Agent
[0071] Take 5 g of refined polyprenol samples and dissolve them in 100 ml of n-hexane solution. Take POCl 3 Dissolve 2.8ml of solvent in 100ml of n-hexane solution, transfer it to a 500ml three-neck flask, stir under ice bath at a stirring speed of 100-800r / min, dissolve 4.2ml of triethylamine in 30ml of n-hexane solution, slowly add triethylamine dropwise Put the amine n-hexane solution into the reactor at a rate of 1-5ml / min. During the dropping process, when a large amount of white mist is generated, stir in vacuum at a stirring speed of 100-800r / min, with a vacuum degree greater than 600mmHg, and react for 30min.
[0072] Then slowly drop 100ml of polypentenol n-hexane solution into the reactor, the dropping speed is 1-5ml / min., the stirring speed is 50-800r / min, react in ice bath for 1 hour, and the reaction product is polypentenyl chlorophosphoric acid Esters mixt...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com