Sulfur-based autotrophic microorganism denitrification material as well as preparation and application methods thereof
The technology of an autotrophic microorganism and an application method is applied in the field of preparation of autotrophic microorganism denitrification materials, and can solve the problems of low density of sulfur particles, separation of sulfur particles and carbonate particles, and increased loss, etc., so as to improve the biological response. Activity, improve the efficiency of electron transfer, improve the effect of mechanical strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0033] The sulfur and lime powder are mixed evenly according to the dry base mass ratio of 8:1 to obtain the mixed material; The mixed material is added to the hopper of the molding machine, and the sulfur is melted in the molding machine heated to 125 ~ 140 °C, and the mixed material becomes a viscous plastic flow state; Then, the material is extruded by the molding machine, cut and cooled, and the particles with a diameter of 5 mm and a length of about 10 mm are obtained. The above-mentioned molded particles are put into the tray and sprayed with water to maintain a continuous wetting state, natural carbonation in the air for 20 days, and the pH value of the aqueous solution soaked in the particles is 6.8, which meets the requirements and obtains the sulfur-based autotrophic microbial denitrification material.
[0034]The prepared sulfur-based autotrophic microbial denitrification material was mixed with limestone particles with a particle size of 3-6 mm according to the mass ra...
Embodiment 2
[0036] The sulfur and lime powder are mixed uniformly according to the dry base mass ratio of 7:1 to obtain the mixed material; The mixed material is added to the hopper of the molding machine, and the sulfur is melted in the molding machine heated to 130~ 140 °C, and the mixed material becomes a viscous plastic flow state; Then, the material is extruded by the molding machine, cut and cooled, and the particles with a diameter of 5 mm and a length of about 10 mm are obtained. The above-mentioned molded particles are put into the tray and sprayed with water to maintain a continuous wetting state, natural carbonation in the air for 20 days, and the pH value of the aqueous solution soaked in the particles is 6.8, which meets the requirements and obtains the sulfur-based autotrophic microbial denitrification material.
[0037] The prepared sulfur-based autotrophic microbial denitrification material was mixed with dolomite particles with a particle size of 3-6 mm according to the mass ...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
length | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com