Embodiment 1
[0062] (1) Add 1.14g of CBMA into 0.5ml of deionized aqueous solution and stir fully to form a uniform mixed solution;
[0063] (2) Add 1.4 μl of DMAEMA into 0.5 ml of triethylene glycol, stir well to form a uniform mixed solution;
[0064] (3) At room temperature, quickly transfer the homogeneous mixed solution formed in step (2) to the solution in step (1), and add 10 mg of initiator I-2959;
[0065] (4) Add 600 mg of benzophenone into 30 ml of isopropanol / acetone=9:1 mixed solvent;
[0066] (5) Immerse the invisible braces in the mixed solvent obtained in step (4) for 3 minutes;
[0067] (6) Coating the mixed solution obtained in step (3) on the invisible correction material obtained in step (5), and reacting for 60 minutes under ultraviolet irradiation.
[0068] (7) Soak the material obtained in step (6) in deionized water for 24 hours.
Embodiment 2
[0070] (1) Add 1.15g of CBMA into 0.5ml of deionized aqueous solution, stir well to form a uniform mixed solution;
[0071] (2) Add 1.4 μl of DMAEMA into 0.5 ml of triethylene glycol, stir well to form a uniform mixed solution;
[0072] (3) At room temperature, quickly transfer the homogeneous mixed solution formed in step (2) to the solution in step (1), and add 10 mg of initiator I-2959;
[0073] (4) Add 600 mg of benzophenone into 30 ml of isopropanol / acetone=9:1 mixed solvent;
[0074] (5) Immerse the invisible braces in the mixed solvent obtained in step (4) for 3 minutes;
[0075] (6) Coating the mixed solution obtained in step (3) on the invisible correction material obtained in step (5), and reacting for 60 minutes under ultraviolet irradiation.
[0076] (7) Soak the material obtained in step (6) in deionized water for 24 hours.
Embodiment 3
[0078] (1) Add 1.16g of CBMA into 0.5ml of deionized aqueous solution and stir fully to form a uniform mixed solution;
[0079] (2) Add 1.4 μl of DMAEMA into 0.5 ml of triethylene glycol, stir well to form a uniform mixed solution;
[0080] (3) At room temperature, quickly transfer the homogeneous mixed solution formed in step (2) to the solution in step (1), and add 10 mg of initiator I-2959;
[0081] (4) Add 600 mg of benzophenone into 30 ml of isopropanol / acetone=9:1 mixed solvent;
[0082] (5) Immerse the invisible braces in the mixed solvent obtained in step (4) for 3 minutes;
[0083] (6) Coating the mixed solution obtained in step (3) on the invisible correction material obtained in step (5), and reacting for 60 minutes under ultraviolet irradiation.
[0084] (7) Soak the material obtained in step (6) in deionized water for 24 hours.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com