Method for reconstructing waterproof layer through minimally invasive technology
A waterproof layer and technology, applied in building structures, building components, protection devices, etc., can solve the problems of large amount of materials, long construction period and complicated operation.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0030] A method for rebuilding a waterproof layer with a minimally invasive technique, the scheme of which is:
[0031] Step 1. Seal the cracks, clean up the cracks on the building surface that need to be repaired, and then seal the cracks with fast-curing mortar;
[0032] Step 2: Drill holes, drill grouting holes on the building surface that needs to be repaired, the number of holes to be drilled is 4 pcs / m 2 , and bury the grouting needle in the grouting hole;
[0033] Step 3: Inject the filler, inject the back filler from the grouting hole, and prepare the back filler according to the following method:
[0034] Stir and mix 20kg methacrylic acid, 10kg styrene, 15kg castor oil maleate and 0.1kg diallyl bisphenol A, then add 0.8kg initiator, stir and mix evenly, slowly add to 30kg butyl glycol In the ether, control the addition within 30 minutes, control the temperature to 90°C and react for 3 hours. After the reaction is completed, add 15.6kg of expanded perlite, 10.2kg of...
Embodiment 2
[0043] A method for rebuilding a waterproof layer with a minimally invasive technique, the scheme of which is:
[0044] Step 1. Seal the cracks, clean up the cracks on the building surface that need to be repaired, and then seal the cracks with fast-curing mortar;
[0045] Step 2: Drill holes, drill grouting holes on the building surface to be repaired, the number of holes to be drilled is 6 pcs / m 2 , and bury the grouting needle in the grouting hole;
[0046] Step 3: Inject the filler, inject the back filler from the grouting hole, and prepare the back filler according to the following method:
[0047] Stir and mix 25kg methacrylic acid, 13kg styrene, 18kg castor oil maleate and 0.3kg diallyl bisphenol A, then add 1kg initiator, stir and mix evenly, slowly add to 40kg butyl glycol ether Control the addition within 60 minutes, control the temperature to 100°C and react for 4 hours. After the reaction is completed, add 22.4kg of expanded perlite, 13.6kg of mica powder, 4.8kg ...
Embodiment 3
[0056] A method for rebuilding a waterproof layer with a minimally invasive technique, the scheme of which is:
[0057] Step 1. Seal the cracks, clean up the cracks on the building surface that need to be repaired, and then seal the cracks with fast-curing mortar;
[0058] Step 2: Drill holes, drill grouting holes on the building surface to be repaired, the number of holes to be drilled is 8 / m 2 , and bury the grouting needle in the grouting hole;
[0059] Step 3: Inject the filler, inject the back filler from the grouting hole, and prepare the back filler according to the following method:
[0060] Stir and mix 30kg methacrylic acid, 15kg styrene, 22kg castor oil maleate and 0.5kg diallyl bisphenol A, then add 1.2kg initiator, stir and mix evenly, slowly add to 50kg butyl glycol In the ether, control the addition within 120 minutes, control the temperature to 110°C and react for 6 hours. After the reaction is completed, add 32.2kg of expanded perlite, 16.6kg of mica powder,...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com