A non-ferrous metal, copper-lead technology, applied in chemical instruments and methods, flotation, wet separation, etc., can solve the problem of low separation efficiency, high mutual content of concentrate, and inability to obtain single lead concentrate, zinc concentrate, etc. problem, to avoid separation difficulty and reduce the effect of separation difficulty
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0014] Embodiment 1, a comprehensive recovery process of iron symbiotic non-ferrous metals copper, lead and zinc, including the following steps, step 1, adding lime to the slurry of iron dressing tailings to adjust the pH value of the slurry to 10, grinding it with a ball mill, and then adding copper sulfate 20 -30 g / t raw ore, butyl xanthate 10-20 g / t raw ore, terpineol oil 20-30 g / t raw ore are stirred and then mixed with copper, lead and zinc for roughing to obtain copper, lead and zinc mixed rough concentrate, which is Add lime to the lead-zinc mixed coarse concentrate until the pH value is 12, then carry out copper-lead-zinc mixed concentration to obtain copper-lead-zinc concentrate slurry; step 2, add the copper-lead-zinc concentrate slurry in step 1 to 50-100 g / m of activated carbon 1 ton raw ore, sodium sulfide 50-100 g / t raw ore, after regrinding, add sodium metabisulfite and dilute sulfuric acid and stir for 5 minutes, so that the pH value of the pulp is 6-6.5, the ad...
Embodiment 2
[0015] Embodiment 2, according to the comprehensive recovery process of a kind of iron symbiotic non-ferrous metal copper, lead and zinc described in embodiment 1, add copper sulfate 25 grams / ton raw ore, butyl xanthate 15 grams / ton raw ore, pine Alcohol oil 25 g / ton.
Embodiment 3
[0016] Embodiment 3, according to the comprehensive recovery process of iron symbiotic non-ferrous metals copper, lead and zinc described in embodiment 1 or 2, 80 g / ton of activated carbon and 80 g / ton of sodium sulfide are added in the step 2.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com