Hardened decorative film and preparation method thereof
A decorative film and hardened film technology, applied in the field of hardened decorative film and its preparation, can solve the problems of increased packaging cost, non-stain resistance, and non-scratch resistance, and achieve the effects of improving production efficiency, good scratch resistance, and reducing waste
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0028] A hardened decorative film includes a base material, the base material is a first PET film, a PVC film, and a second PET film in sequence from the inside to the outside; the surface of the second PET film has a surface hardened film.
[0029] The surface hardening film is made by coating with UV curing liquid, and its thickness is 4 μm. The raw material components of the UV hardening solution are as follows, in parts by weight, 43 parts of modified water-based acrylate, 40 parts of ethyl acetate, 11 parts of nano-silica, 1 part of photoinitiator, 0.8 parts of fluorine-containing antifouling additive, Fluorine-modified acrylic leveling agent 0.5 parts.
[0030]A method for preparing a hardened decorative film, comprising the following steps: (1) preparing a UV hardening solution; taking carbon nanotube powder, adding hydrogen peroxide solution, and reacting for 2.5 hours; centrifuging and washing with deionized water; the temperature is 80°C drying at lower temperature;...
Embodiment 2
[0039] A hardened decorative film includes a base material, the base material is a first PET film, a PVC film, and a second PET film in sequence from the inside to the outside; the surface of the second PET film has a surface hardened film.
[0040] The surface hardening film is made by coating with UV curing liquid, and its thickness is 5 μm. The raw material components of the UV hardening solution are as follows, in parts by weight, 51 parts of modified water-based acrylate, 49 parts of ethyl acetate, 13 parts of nano-silica, 2 parts of photoinitiator, 1.1 parts of fluorine-containing antifouling additive, 0.7 parts of fluorine-modified acrylic leveling agent.
[0041] A method for preparing a hardened decorative film, comprising the following steps: (1) preparing a UV hardening solution; taking carbon nanotube powder, adding hydrogen peroxide solution, and reacting for 2.7 hours; centrifuging and washing with deionized water; the temperature is 81°C drying at lower tempera...
Embodiment 3
[0050] A hardened decorative film includes a base material, the base material is a first PET film, a PVC film, and a second PET film in sequence from the inside to the outside; the surface of the second PET film has a surface hardened film.
[0051] The surface hardening film is made by coating with UV curing liquid, and its thickness is 6 μm. The raw material components of the UV hardening solution are as follows, in parts by weight, 57 parts of modified water-based acrylate, 60 parts of ethyl acetate, 17 parts of nano silicon dioxide, 3 parts of photoinitiator, 1.5 parts of fluorine-containing antifouling additive, Fluorine modified acrylic leveling agent 1 part.
[0052] A method for preparing a hardened decorative film, comprising the following steps: (1) preparing a UV hardening solution; taking carbon nanotube powder, adding hydrogen peroxide solution, and reacting for 3 hours; centrifuging and washing with deionized water; drying; adding sodium dodecylbenzenesulfonate ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com