Application of Prussian blue in preparation of medicines for treating acute pancreatitis
A technology of acute pancreatitis and Prussian blue, applied in the application field of Prussian blue, can solve the problems of limited clinical application, complicated preparation and treatment process, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0048] (1) Add 2400mg of potassium ferricyanide and 5g of polyvinylpyrrolidone (PVP) into 60mL of 2M hydrochloric acid, and stir magnetically until a clear solution is obtained;
[0049] (2) Transfer the above-mentioned clear solution to an electric cooker, and react for 72 hours at a temperature of 200° C. and a pressure of 10 MPa;
[0050] (3) Take out and cool to room temperature, centrifuge, wash with deionized water for several times, and freeze-dry to obtain Prussian blue nanoparticles with a size of 2-400nm.
Embodiment 2
[0052] (1) Add 300 mg of potassium ferricyanide and 3 g of polyvinylpyrrolidone (PVP) to 50 mL of 2M hydrochloric acid, and stir magnetically until a clear solution is obtained;
[0053] (2) Transfer the above-mentioned clear solution to an electric cooker, and react for 48 hours at a temperature of 100° C. and a pressure of 20 MPa;
[0054] (3) Take out and cool to room temperature, centrifuge, wash with deionized water for several times, and freeze-dry to obtain Prussian blue nanoparticles with a size of 2-400nm.
Embodiment 3
[0056] Step A) Add 3960 mg of potassium ferricyanide and 35 g of polyvinylpyrrolidone (PVP) into 100 mL of 2M hydrochloric acid, and stir magnetically until a clear mixed solution is obtained;
[0057] Step B) Transfer the mixed solution to an oven at 80°C, age for 20 hours, take it out, cool to room temperature, centrifuge, wash with deionized water several times, dissolve in 50mL of 1.5M hydrochloric acid and set aside;
[0058] Step C) Transfer 20mL of the above solution to a hydrothermal kettle, place in an electric furnace, age at 120°C for 4h, take it out and cool to room temperature, centrifuge, wash with deionized water several times, and freeze-dry to obtain a pore size in the range of 3-20nm The inner size is 30-200nm mesoporous Prussian blue nanoparticles.
PUM
Property | Measurement | Unit |
---|---|---|
Size | aaaaa | aaaaa |
Specific surface area | aaaaa | aaaaa |
Aperture | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com