A production method and production device technology, applied in the field of textile yarns, can solve the problems of not being easy to wear next to the body, itching, poor releaseability, etc., and achieve the effects of obvious elasticity and functional characteristics, easy protection or sealing, and good shape retention
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0044] The preparation method of roving B in the present embodiment is as follows:
[0045] The raw material fibers of the roving B are 40% stretch-elastic short fibers and 60% cotton; 10wt% of the raw cotton fibers are indigo;
[0046] Described adopting the method preparation comprising the following steps to obtain:
[0047] 1) Shu elastic silk elastic short fiber and cotton fiber are mixed to form mixed raw materials;
[0048] 2) The mixed raw materials are made into laps in the cleaning process, and the lap weight is 420 g / m; the lap length is 36 meters;
[0049] 3) Comb the lap into slivers on the carding machine; raw sliver weight is 22 g / 5 m; doffer speed is 20 rpm; distance between cover plate and cylinder card clothing is 8, 7, 6, 6, 7 ;
[0050] 4) The raw sliver is combined and drafted three times on the draw frame to form a sliver; the sliver final weight is 20.5g / 5m; the combined number is 8; the final draft is 8.59 times, and the speed is 320m / min;
[0051] ...
Embodiment 2
[0066] In this example, the melange spun core-spun yarn is used for fine-count wool-containing knitted sweaters.
[0067] Roving B is prepared by the method comprising the following steps:
[0068] 1) The raw material fiber of roving B is: 60wt% wool, 40wt% cotton; Cotton fiber has 10wt% black;
[0069] 2) It is also possible to pre-treat the wool fiber to prevent its electrostatic effect;
[0070] 3) mixing wool fiber and cotton fiber to form mixed fiber;
[0071] 4) The mixed fibers are made into laps in the cleaning process, and the lap weight is 420 g / m; the lap length is 36 meters;
[0072] 5) Comb the laps into raw slivers on the carding machine; raw sliver weight is 18-24g / 5m; doffer speed is 15-22 rpm; distance between cover plate and cylinder clothing is 8,7,6 ,6,7;
[0073] 6) The raw sliver is combined and drafted three times on the drawing frame to form a sliver; the final weight of the sliver is 20.5g / 5m; the combined number is 8; the draft is 8.5 times, and t...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com