Embodiment 1
[0034] A rare earth mine in Sichuan, the ore contains 4.16% REO, the main rare earth minerals are bastnaesite, pericite, allanite, iron minerals are hematite, limonite, and gangue minerals are mainly quartz and fluorite , barite, calcite, feldspar, sodium iron amphibole, muscovite, etc.
[0035] The beneficiation steps are as follows:
[0036] Pretreatment: mix the ore with water, the ore mass percentage concentration is 20%, and grind the ore to -0.074mm in a ball mill to account for 90%.
[0037] Adding agents: sodium hydroxide: add 100 grams per ton of ore; water glass: add 4000 grams per ton of ore; hydroxamic acid: add 4000 grams per ton of ore; pinitol oil: add 30 grams per ton of ore.
[0038] Stirring: Add the above-mentioned agents into the slurry in order, and stir while adding. After the last agent is added, continue to stir for 5 minutes.
[0039] Flotation: 3-10 minutes of flotation to obtain the rough concentrate of rare earth ore, and the rough concentrate is ...
Embodiment 2
[0042] A rare earth mine in Shandong, the ore contains 3.22% REO, the main rare earth minerals are bastnaesite, bastnaesite, ceriapatite, monazite and so on. Gangue minerals include calcite, barite, sodium iron amphibole, quartz, fluorite, mica and so on.
[0043] The beneficiation steps are as follows:
[0044] Pretreatment: mix the ore and water, the ore mass percentage concentration is 70%, and grind the ore to -0.074mm in a ball mill to account for 60%.
[0045]Adding agents: sodium hydroxide: add 900 grams per ton of ore; water glass: add 2000 grams per ton of ore; hydroxamic acid: add 1500 grams per ton of ore; pinitol oil: add 200 grams per ton of ore.
[0046] Stirring: Add the above medicaments into the slurry in order, and stir while adding. After the last medicament is added, continue to stir for 3 minutes.
[0047] Flotation: 3-10 minutes of flotation to obtain rough concentrate of rare earth ore, and the rough concentrate is subjected to 2 times of beneficiation...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com