A magnesium-aluminum spinel and positive electrode material technology, which is applied in the sagger for sintering lithium battery positive electrode materials and its preparation, can solve the problems of low thermal shock performance, poor corrosion resistance, and low material strength, and achieve heat resistance Good shock resistance, improved thermal shock resistance and high strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0035] A sagger for sintering lithium battery positive electrode materials based on magnesium aluminum spinel sol and a preparation method thereof. The steps of the preparation method described in this embodiment are:
[0036] Step 1: Mix 20-22wt% magnesium nitrate, 18-20wt% aluminum nitrate and 60-61wt% industrial alcohol, and stir at 60°C for 1-1.5h to obtain magnesium aluminum spinel sol.
[0037] Step 2, mix 25-27wt% mullite particles, 28-30wt% cordierite particles, 28-30wt% andalusite particles, 3-4wt% magnesium aluminum spinel sol, 4-7wt% The Guangxi white clay is mixed with 5-7wt% silicon micropowder, and stirred for 8-10 minutes to obtain the mixture.
[0038] Step 3: Machine press the mixture under the condition of 100-105 MPa, dry it at 90-110°C for 20-25 hours, and then keep it at 1300-1325°C for 3-4 hours to obtain a magnesium-aluminum tip A sagger for sintering the lithium battery cathode material of spar sol.
Embodiment 2
[0040] A sagger for sintering lithium battery positive electrode materials based on magnesium aluminum spinel sol and a preparation method thereof. The steps of the preparation method described in this embodiment are:
[0041] Step 1: Mix 21-23wt% magnesium nitrate, 17-19wt% aluminum nitrate and 60-61wt% industrial alcohol, and stir at 60°C for 1-1.5h to obtain magnesium aluminum spinel sol.
[0042] Step 2, mix 26-28wt% of mullite particles, 27-29wt% of cordierite particles, 27-29wt% of andalusite particles, 4-5wt% of the magnesium aluminum spinel sol, 4-7wt% The Guangxi white mud is mixed with 4-6wt% silicon micropowder, and stirred for 8-10 minutes to obtain the mixture.
[0043] Step 3: Machine press the mixture under the condition of 105-110MPa, dry at 90-110°C for 20-25 hours, and then keep it warm at 1325-1350°C for 3-4 hours to obtain a magnesium-aluminum tip A sagger for sintering the lithium battery cathode material of spar sol.
Embodiment 3
[0045] A sagger for sintering lithium battery positive electrode materials based on magnesium aluminum spinel sol and a preparation method thereof. The steps of the preparation method described in this embodiment are:
[0046] Step 1: Mix 22-24wt% magnesium nitrate, 16-18wt% aluminum nitrate and 60-61wt% industrial alcohol, and stir at 60°C for 1-1.5h to obtain magnesium aluminum spinel sol.
[0047] Step 2, mix 27~29wt% of mullite particles, 26~28wt% of cordierite particles, 26~28wt% of andalusite particles, 5~6wt% of the magnesium aluminum spinel sol, 4~7wt% The Guangxi white clay is mixed with 3-5wt% silicon micropowder, and stirred for 8-10 minutes to obtain the mixture.
[0048] Step 3: Machine press the mixture under the condition of 110-115MPa, dry at 90-110°C for 20-25 hours, and then keep it warm at 1350-1375°C for 3-4 hours to obtain a magnesium-aluminum tip A sagger for sintering the lithium battery cathode material of spar sol.
PUM
Property | Measurement | Unit |
---|---|---|
density | aaaaa | aaaaa |
particle size | aaaaa | aaaaa |
density | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com