A soil improver and improver technology, applied in the field of soil remediation, can solve the problems of cumbersome and complex calculations, high quality and precision requirements for mixing equipment and metering equipment, and achieve simple calculations, low requirements, and improved passivation The effect of heavy metal abilities
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0070] Soil conditioner, this conditioner comprises the following components by weight percentage:
[0071] Copper tailings 60%
[0072] Fluorite tailings 30%
[0073] Talc 6%
[0074] Carboxymethyl Cellulose 4%
[0075] Among them, the particle size of each component in the modifier is less than 0.5mm, accounting for more than 90%;
[0076] The preparation method of soil conditioner comprises the following steps:
[0077] Step 1. Weigh each component and mix well;
[0078] Step 2, the mixture obtained in step 1 is made into 5-10mm pellets;
[0079] Step 3, calcining the pellets at a temperature of 1300° C. for 2.5 hours;
[0080] Step 4, cooling and activating the pellets, and ball milling to 100 mesh to obtain a soil conditioner.
[0081] Wherein, when the particle size of more than 10% of the added tailings is larger than 0.5 mm, ball milling can be carried out in step 1 first, and ball milling is performed until more than 90% of the particle size of each component i...
Embodiment 2
[0083] Soil conditioner, this conditioner comprises the following components by weight percentage:
[0084] Copper tailings 50%
[0085] Fluorite tailings 27%
[0086] Talc 20%
[0087] Carboxymethyl Cellulose 3%
[0088] Among them, the particle size of each component in the modifier is less than 0.5mm, accounting for more than 90%;
[0089] Soil conditioner preparation methods such as figure 1 shown, including the following steps:
[0090] Step 1. Weigh each component and mix well;
[0091] Step 2, the mixture obtained in step 1 is made into 50-100mm pellets;
[0092] Step 3, calcining the pellets at a temperature of 1150° C. for 2.0 hours;
[0093] Step 4, cooling and activating the pellets, and ball milling to 50 mesh to obtain a soil conditioner.
[0094] Wherein, when the particle size of more than 10% of the added tailings is larger than 0.5 mm, ball milling can be carried out in step 1 first, and ball milling is performed until more than 90% of the particle siz...
Embodiment 3
[0096] Soil conditioner, this conditioner comprises the following components by weight percentage:
[0097] Copper tailings 40%
[0098] Fluorite tailings 40%
[0099] Talc 15%
[0100] Carboxymethyl Cellulose 5%
[0101] Among them, the particle size of each component in the modifier is less than 0.5mm, accounting for more than 90%;
[0102] The preparation method of soil conditioner comprises the following steps:
[0103] Step 1. Weigh each component and mix well;
[0104] Step 2, the mixture obtained in step 1 is made into 5-10mm pellets;
[0105] Step 3, calcining the pellets at a temperature of 1000° C. for 1.5 hours;
[0106] Step 4, cooling and activating the pellets, and ball milling to 60 mesh to obtain a soil conditioner.
[0107] Wherein, when the particle size of more than 10% of the added tailings is larger than 0.5 mm, ball milling can be carried out in step 1 first, and ball milling is performed until more than 90% of the particle size of each component i...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com