Bamboo fiber, bast fiber and wool blended yarn and production method thereof
A production method and technology of blended yarn, which can be used in yarn, textile and papermaking, chemical production of bast fibers, etc., can solve the problems of poor wrinkle resistance and wear resistance, poor elasticity, and low wet strength.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] Spinning 60 N Bamboo 40 hemp 20 wool 40 blended yarn is formed by blending bamboo fiber, hemp fiber and wool fiber, 40% bamboo fiber, 20% hemp fiber and 40% wool fiber in the yarn, and the "%" is a mass percentage. The spinnable count is 60 N .
[0020] Its production method comprises the following steps:
[0021] (1) According to the product requirements, the raw ramie hemp after scraping is selected, and it is made into dry hemp after degumming, and the dry hemp is softened by a flax softening machine and then added to the wet oil (the amount of oil is 10%, and the oil formulation is tea oil: kerosene :alkali:water=40:60:0.5:400, which is the mass ratio), after weighing, stacking, pulling, and loosening (the dry weight of the feed is 795 g / m, and the dry weight of the output is 72.43 g / m) , combing hemp (output dry weight 25.65 g / m), two pre-merging, combing, pre-combing, and combing to make ramie combed sliver, one pre-combing, and at the same time control the qua...
Embodiment 2
[0032] Spinning 36 N Bamboo 30 hemp 25 wool 45 blended yarn is formed by blending bamboo fiber, hemp fiber and wool fiber, 30% bamboo fiber in the yarn, 25% hemp fiber and 45% wool fiber, and the "%" is a mass percentage. The spinnable count is 36 N .
[0033] Its production method comprises the following steps:
[0034] (1) According to the product requirements, the raw ramie hemp after scraping is selected, and it is made into dry hemp after degumming, and the dry hemp is softened by a flax softening machine and then added to the wet oil (the amount of oil is 10%, and the oil formulation is tea oil: kerosene :Alkali:Water=40:60:0.5:400, which is the mass ratio), after weighing, stacking, pulling, and loosening (the dry weight of the feed is 815 g / m, and the dry weight of the output is 73.62 g / m) , combing hemp (output dry weight 27.63 g / m), two pre-merging, combing, pre-combing, and combing to make ramie combed sliver, one pre-combing, and at the same time control the qua...
Embodiment 3
[0045] Spinning 10 N Bamboo 25 hemp 15 wool 60 blended yarn is formed by blending bamboo fiber, hemp fiber and wool fiber, 25% bamboo fiber in the yarn, 15% hemp fiber and 60% wool fiber, and the "%" is a mass percentage. The spinnable count is 10 N .
[0046]Its production method comprises the following steps:
[0047] (1) According to the product requirements, the raw ramie hemp after scraping is selected, and it is made into dry hemp after degumming, and the dry hemp is softened by a flax softening machine and then added to the wet oil (the amount of oil is 10%, and the oil formulation is tea oil: kerosene :alkali:water=40:60:0.5:400, which is the mass ratio), after weighing, stacking, pulling, and loosening (feeding dry weight is 830 g / m, output dry weight is 75.26 g / m) , combing hemp (output dry weight 28.35 g / m), two pre-merging, combing, pre-combing, and combing to make ramie combed sliver, one pre-combing, and at the same time control the quantitative 23.5 of the he...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com