A technology of lignosulfonate and staining, which is applied in the field of preparation of lignosulfonate and low-contamination lignosulfonate, and can solve the problems of unrealized resource utilization, underutilization, and pollution To achieve the effect of realizing waste utilization, good dispersion and reducing environmental pollution
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0028] A method for preparing low-contamination lignin sulfonate from caustic soda pulping waste liquor, comprising the following steps:
[0029] First, the waste liquid is left to stand for 1 hour, and the water-insoluble matter and cellulose impurities in the pulping waste liquid by the caustic soda method are removed by using a disc filter.
[0030] The ultrafiltration membrane filtration equipment is used to concentrate the caustic soda pulping waste liquid, and the concentration of the caustic soda pulping waste liquid is increased from 8wt% to 15wt%.
[0031] Use 10wt% sodium sulfite and 10wt% paraformaldehyde at 90°C and pH=9.2 for 4 hours in the concentrated solution, and carry out sulfonation and condensation reactions on the concentrated solution to produce lignin sulfonate with high dispersibility and heat resistance salt.
[0032] The sulfonated concentrated solution was reacted with 4 wt % hydrogen peroxide at 50° C. for 2 hours to reduce the staining property of...
Embodiment 2
[0036] A method for preparing low-contamination lignin sulfonate from caustic soda pulping waste liquor, comprising the following steps:
[0037] First, the waste liquid is left to stand for 1 hour, and the water-insoluble matter and cellulose impurities in the pulping waste liquid by the caustic soda method are removed by using a disc filter.
[0038] The nanofiltration membrane filtration equipment is used to concentrate the caustic soda pulping waste liquid, and the concentration of the caustic soda pulping waste liquid is increased from 10wt% to 20wt%.
[0039] Use 13wt% sulfur dioxide and 15% formaldehyde in the concentrate to react at 95°C and pH=12.8 for 3 hours, and carry out sulfonation and condensation reactions on the concentrate to produce lignosulfonate with high dispersibility and heat resistance .
[0040] The sulfonated concentrated solution was reacted with 5 wt% hydrogen peroxide at 60° C. for 1 hour to reduce the staining property of lignosulfonate.
[004...
Embodiment 3
[0044] A method for preparing low-contamination lignin sulfonate from caustic soda pulping waste liquor, comprising the following steps:
[0045] First, the waste liquid is left to stand for 1 hour, and the water-insoluble matter and cellulose impurities in the pulping waste liquid by the caustic soda method are removed by using a disc filter.
[0046] The nanofiltration membrane filtration equipment is used to concentrate the caustic soda pulping waste liquid, and the concentration of the caustic soda pulping waste liquid is increased from 15wt% to 30wt%.
[0047] Use 30wt% sodium bisulfite and 35wt% formaldehyde in the concentrated solution to react for 5 hours at 80°C and pH=8.0, and carry out sulfonation and condensation reactions on the concentrated solution to produce high dispersion, heat resistance, and low Staining lignosulfonates.
[0048]Sodium chlorite with an amount of 8 wt% of the concentrated solution was used to react at 80° C. for 4 hours to react the sulfona...
PUM
Property | Measurement | Unit |
---|---|---|
Degree of sulfonation | aaaaa | aaaaa |
Degree of sulfonation | aaaaa | aaaaa |
Degree of sulfonation | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com