Safety fabric and manufacture method thereof
A fabric and safe technology, applied in the field of safe fabrics and its preparation, can solve problems such as weakening of bulkiness, allergies, and hardening of fabrics, and achieve the effect of improving bulkiness, good bulkiness, and good bulkiness
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0026] A method for preparing a safe fabric, comprising the steps of:
[0027] S1. Raw material preparation: twist the cotton wadding with twist and water-soluble fiber to form a raw material thread, and the direction of twisting is opposite to the direction of the twist of the cotton wadding;
[0028] S2. Textile forming: the batting layer 3 formed by weaving the raw material thread is arranged between the first cotton layer 1 and the second cotton layer 2 to obtain an intermediate fabric;
[0029] S3. Washing: washing the obtained intermediate fabric to obtain a final fabric.
[0030] In S1, the mass ratio of the water-soluble fiber to the cotton wool in the raw material line is 1:10-1:100. It is set according to the thickness of the cotton-wool layer 3 and whether it is soluble during water-soluble treatment.
[0031] In S2, the knitting circular weft knitting machine is used, the cotton thread is used as the incoming thread of the first cotton layer 1 and the second cott...
Embodiment 1
[0036] S1. Raw material preparation: Cotton batts with a twist of 20-30 twists (Tex twist coefficient) and water-soluble fibers are mixed and twisted into raw material threads. The direction of twisting is opposite to that of the cotton batts, and the twist is 18 twists. , the mass ratio of the water-soluble fiber of the raw material line to the cotton wool is 1:10;
[0037] S2. Textile molding: use a circular weft knitting machine, use the cotton thread as the incoming thread of the first cotton layer 1 and the second cotton layer 2, and use the raw material thread as the incoming thread of the cotton layer 3, and use the chain link process on the first cotton cloth A hooking line 4 is set between the layer 1 and the second cotton layer 2, and a first cotton layer 1, a cotton layer 3, and a second cotton layer 2 are spun from top to bottom to obtain an intermediate fabric;
[0038] S3. Washing: the obtained intermediate fabric was washed at a temperature of 80°C for 3 hours, ...
Embodiment 2
[0040] S1. Raw material preparation: Cotton batts with a twist of 25-30 twists (Tex twist coefficient) and water-soluble fibers are mixed and twisted into raw material threads. The direction of twisting is opposite to that of the cotton batts, and the twist is 24 twists. , the mass ratio of the water-soluble fiber of the raw material line to the cotton wool is 1:100;
[0041] S2. Textile forming: use a circular weft knitting machine, use the cotton thread as the incoming thread of the first cotton layer 1 and the second cotton layer 2, and use the raw material thread as the incoming thread of the cotton layer 3, and weave it in a sequence from top to bottom The first cotton cloth layer 1, the batting layer 3, and the second cotton cloth layer 2 are set to obtain the middle fabric;
[0042] S3. Washing: washing the obtained intermediate fabric at a temperature of 100° C. for 1 hour, and the mass ratio of water-soluble fibers to cotton wool in the cotton-wool layer 3 in the fina...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com