A single crystal diamond, stability technology, applied in the direction of single crystal growth, single crystal growth, chemical instruments and methods, etc., can solve the problem of more than single crystal diamond, single crystal diamond seed crystal heat dissipation deterioration, interruption of single crystal diamond growth, etc. problems, to achieve the effect of simple processing, flexible use, and improved heat dissipation capacity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0031] The size of the single crystal diamond seed crystal is: length 8mm, width 8mm, thickness 0.4mm. Open a small groove on the sample table where the single crystal diamond seed crystal is placed. The size of the small groove is between 3mm*3mm-6mm*6mm. Square or circular or other symmetrical sizes are acceptable, and the requirements are easy to process; the groove depth depends on Processing requirements control the depth between 0.2mm-0.4mm. Then drop a certain amount of liquid metal into the tank until it nearly fills the small tank or slightly overflows a small amount. Put the transparent single crystal diamond seed crystal on the liquid metal, and you can observe the wettability between the liquid metal and the single crystal diamond seed crystal. Full surface contact.
Embodiment 2
[0033] The size of the single crystal diamond seed crystal is: length 8mm, width 8mm, thickness 0.4mm. Open a large groove slightly larger than the length and width of the single crystal diamond at the position where the single crystal diamond seed crystal is placed on the sample stage, and then open a small groove at the bottom of the large groove. The size of the large groove is between 9mm*mm-12mm*12mm, the size of the small groove is between 3mm*3mm-6mm*6mm, square or round or other symmetrical sizes are acceptable, and it is required to be easy to process; this is due to the early drawing During the vacuum or later degassing process, the single crystal diamond seed crystal may be displaced due to the air flow surge during the gas flow inside the reaction chamber. Open a large groove and place the single crystal diamond seed crystal in the large groove to avoid large Amplitude displacement. Open a small groove again, drop into liquid metal, and mode is identical with embo...
PUM
Property | Measurement | Unit |
---|---|---|
solidification point | aaaaa | aaaaa |
boiling point | aaaaa | aaaaa |
size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com