An extruded board, an environmentally friendly technology, applied in the field of boards, can solve the problems that the texture of organic polymer materials cannot be reflected, the quality of inorganic insulation materials is heavy, and it takes a long time to achieve uniform internal structure dispersion and insulation effects Good, dense effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0014] An environmentally-friendly extruded board and a preparation method thereof. The raw material composition is composed of 65 parts by weight of polystyrene resin, 22 parts of epoxy resin, 14 parts of white carbon black, 12 parts of hollow glass beads, 6 parts of calcium carbonate, 7 parts of silicon carbide, 6 parts of tetrafluorodichloroethane, 4 parts of coconut oil fatty acid diethanolamide, 8 parts of deionized water, and 14 parts of argon.
[0015] The preparation method is as follows:
[0016] A. Perform high-temperature fusion and polycondensation of polystyrene resin and epoxy resin at a temperature of 1050°C. Add white carbon black, silicon carbide and hollow glass beads for stirring at a stirring rate of 650r / min. Mixture A;
[0017] B. Add coconut oil fatty acid diethanolamide and tetrafluorodichloroethane into deionized water and stir at a stirring rate of 420r / min. After stirring, the excess water is distilled out to a viscous state to obtain mixture B;
[0018] C....
Embodiment 2
[0020] An environmentally friendly extruded board and a preparation method thereof. The raw material composition is composed of 80 parts by weight of polystyrene resin, 20 parts of epoxy resin, 10 parts of white carbon black, 15 parts of hollow glass beads, 5 parts of calcium carbonate, 7 parts of silicon carbide, 4 parts of tetrafluorodichloroethane, 3 parts of coconut oil fatty acid diethanolamide, 10 parts of deionized water, and 10 parts of argon.
[0021] The preparation method is as follows:
[0022] A. Perform high-temperature fusion and polycondensation of polystyrene resin and epoxy resin at a temperature of 1250°C. Add white carbon black, silicon carbide and hollow glass beads for stirring. The stirring rate is 800r / min. Mixture A;
[0023] B. Add coconut oil fatty acid diethanolamide and tetrafluorodichloroethane into deionized water and stir at a stirring rate of 500r / min. After stirring, the excess water is distilled out to a viscous state to obtain mixture B;
[0024] C...
Embodiment 3
[0026] An environmentally friendly extruded board and a preparation method thereof. The raw materials are composed of 75 parts by weight of polystyrene resin, 24 parts of epoxy resin, 13 parts of white carbon black, 15 parts of hollow glass beads, 7 parts of calcium carbonate, 6 parts of silicon carbide, 5 parts of tetrafluorodichloroethane, 4 parts of coconut oil fatty acid diethanolamide, 8 parts of deionized water, and 16 parts of argon.
[0027] The preparation method is as follows:
[0028] A. Perform high-temperature fusion and polycondensation of polystyrene resin and epoxy resin at a temperature of 1150°C. Add white carbon black, silicon carbide and hollow glass beads for stirring at a stirring rate of 700r / min. After stirring uniformly, obtain Mixture A;
[0029] B. Add coconut oil fatty acid diethanolamide and tetrafluorodichloroethane into deionized water and stir at a stirring rate of 500r / min. After stirring, the excess water is distilled out to a viscous state to obtai...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com