Acid rain sampling, measuring and analyzing instrument
A technology for the measurement and analysis of acid rain, applied in the direction of anti-corrosion coatings, coatings, etc., can solve the problem of unsatisfactory surface finish, and achieve the effect of excellent anti-oxidation and high surface finish
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] A kind of acid rain sampling determination analyzer, it comprises metal casing, and this metal casing is through coating process, and described coating process comprises the steps:
[0026] 1) Put 1-2 parts by weight of lauryltrimethylammonium bromide, 2.5 parts by weight of aluminum oxide, 1.6 parts by weight of dibutyl phthalate, and 0.9 parts by weight of alum into 50 parts by weight of deionized water in sequence, and stir evenly;
[0027] 2) Add 15.5 parts by weight of styrene, 9.9 parts by weight of hydroxypropyl methylcellulose, 1.8 parts by weight of alkylphenol polyoxyethylene ether, and 0.9 parts by weight of potassium tetraborate in turn, and continue to stir until fully mixed and uniform to obtain film treatment solution;
[0028] 3) Put the metal shell into the coating treatment solution for immersion, take it out and dry it.
Embodiment 2
[0030] A kind of acid rain sampling determination analyzer, it comprises metal casing, and this metal casing is through coating process, and described coating process comprises the steps:
[0031] 1) Put 1 part by weight of lauryltrimethylammonium bromide, 2.5 parts by weight of aluminum oxide, 1.6 parts by weight of dibutyl phthalate, and 0.9 parts by weight of alum into 50 parts by weight of deionized water in sequence, and stir evenly;
[0032] 2) Add 15.5 parts by weight of styrene, 9.9 parts by weight of hydroxypropyl methylcellulose, 1.8 parts by weight of alkylphenol polyoxyethylene ether, and 0.9 parts by weight of potassium tetraborate in turn, and continue to stir until fully mixed and uniform to obtain film treatment solution;
[0033] 3) Put the metal shell into the coating treatment solution for immersion, take it out and dry it.
Embodiment 3
[0035] A kind of acid rain sampling determination analyzer, it comprises metal casing, and this metal casing is through coating process, and described coating process comprises the steps:
[0036] 1) Put 2 parts by weight of lauryltrimethylammonium bromide, 2.5 parts by weight of aluminum oxide, 1.6 parts by weight of dibutyl phthalate, and 0.9 parts by weight of alum into 50 parts by weight of deionized water in sequence, and stir evenly;
[0037] 2) Add 15.5 parts by weight of styrene, 9.9 parts by weight of hydroxypropyl methylcellulose, 1.8 parts by weight of alkylphenol polyoxyethylene ether, and 0.9 parts by weight of potassium tetraborate in turn, and continue to stir until fully mixed and uniform to obtain film treatment solution;
[0038] 3) Put the metal shell into the coating treatment solution for immersion, take it out and dry it.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com