Titanium gypsum high-performance concrete building material and preparation method therefor
A technology of high-performance concrete and titanium gypsum, which is applied in the field of gypsum-based cementitious materials, can solve the problems of not considering product performance, difficulty in uniform dispersion, and increasing the crushing process, etc., and achieves good durability, shortened induction period, The effect of simplifying the production process
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0030] Embodiment 1: The present invention provides a kind of titanium gypsum high-performance concrete building material, comprise cementitious material slurry S1 and aggregate S2, it is characterized in that, aggregate S2 is light aggregate, common aggregate one or more than two kinds Combination of any ratio, the ratio between the volume of the cementitious material slurry S1 and the bulk volume of the aggregate S2 is 1:2; wherein the cementitious material slurry S1 is composed of 20 parts of the dry weight of the original titanium gypsum, silicon-aluminum active minerals 70 parts of raw materials, 9 parts of alkaline excited raw materials, and 1 part of acidic excited raw materials; wherein the moisture content of the undisturbed titanium gypsum slag is 50%.
[0031] Wherein the silicon-aluminum active mineral raw material is water-quenched blast furnace slag micropowder (hereinafter referred to as "slag micropowder"), the specific surface area of the micropowder is more ...
Embodiment 2
[0039] Embodiment 2: The present invention provides a kind of titanium gypsum high-performance concrete building material, comprise cementitious material slurry S1 and aggregate S2, it is characterized in that, aggregate S2 is light aggregate, common aggregate one or more than two kinds Combination of any ratio, the ratio between the volume of cementitious material slurry S1 and the bulk volume of aggregate S2 is 1:3; wherein cementitious material slurry S1 is composed of 35 parts of original titanium gypsum dry weight, silicon-aluminum active mineral 55 parts of raw materials, 7 parts of alkaline excited raw materials, and 3 parts of acidic excited raw materials; wherein the moisture content of the undisturbed titanium gypsum slag is 50%.
[0040] Among them, slag micropowder, a silica-alumina active mineral raw material, has a specific surface area of 450M2 / Kg, an activity index of 75% in 7 days, and 105% in 28 days; the alkaline excitation raw material is Portland cement N...
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
cylinder compressive strength | aaaaa | aaaaa |
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com