Looking for breakthrough ideas for innovation challenges? Try Patsnap Eureka!

Production process for wooden door

A production process and wooden door technology, applied in wood processing equipment, manufacturing tools, etc., can solve the problems affecting the smoothness of the paint film, roughness, and uneven wood surface, and achieve the effect of smooth wooden door surface, anti-corrosion, and good anti-corrosion performance

Active Publication Date: 2017-07-14
CHONGQING KUNXIU DOOR & WINDOW
View PDF5 Cites 4 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

Under the action of grinding pressure, these wood hairs often curl up and hide. Once the finishing dye solution, shellac varnish, etc. absorb water or other solvents, they will swell violently and stand upright, resulting in uneven and rough wood surfaces and affecting the paint film. smoothness of

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0024] A kind of production technology of wooden door, comprises the following steps:

[0025] (1) Plate drying: Remove the raw material plates with cracks, and put the raw material plates with flat surface and no cracks into the drying kiln for spray steaming and heating drying. The time of spray steaming is 13 minutes, and the time of heating and drying is 20 days. The moisture content of the board after drying is 10%.

[0026] (2) Pressing the board: Use a planer to press the thickness of the board.

[0027] (3) Cutting: Use a precision panel saw to process the compacted panels into door sides and core panels of specific sizes.

[0028] (4) Sanding: Use a sanding machine to sand the surface of the door core board and the surface of the door edge.

[0029] (5) Group frame: combine the door core board and the door edge to form a wooden door.

[0030] (6) Wood hair removal: a. On the surface of the wooden door, apply a primer layer with a thickness of 0.2mm, a secondary pad...

Embodiment 2

[0037] A kind of production technology of wooden door, comprises the following steps:

[0038] (1) Plate drying: Remove the raw material plates with cracks, and put the raw material plates with flat surface and no cracks into the drying kiln for spray steaming and heating drying. The time of spray steaming is 14 minutes, and the time of heating and drying is 22 days. The moisture content of the board after drying is 11%.

[0039] (2) Pressing the board: Use a planer to press the thickness of the board.

[0040] (3) Cutting: Use a precision panel saw to process the compacted panels into door sides and core panels of specific sizes.

[0041] (4) Sanding: Use a sanding machine to sand the surface of the door core board and the surface of the door edge.

[0042] (5) Group frame: combine the door core board and the door edge to form a wooden door.

[0043] (6) Wood hair removal: a. On the surface of the wooden door, apply a primer layer with a thickness of 0.3mm, a secondary oar...

Embodiment 3

[0050] A kind of production technology of wooden door, comprises the following steps:

[0051] (1) Plate drying: Remove the raw material plates with cracks, and put the raw material plates with flat surface and no cracks into the drying kiln for spray steaming and heating drying. The time of spray steaming is 15 minutes, and the time of heating and drying is 24 days. The moisture content of the board after drying is 12%.

[0052] (2) Pressing the board: Use a planer to press the thickness of the board.

[0053] (3) Cutting: Use a precision panel saw to process the compacted panels into door sides and core panels of specific sizes.

[0054] (4) Sanding: Use a sanding machine to sand the surface of the door core board and the surface of the door edge.

[0055] (5) Group frame: combine the door core board and the door edge to form a wooden door.

[0056] (6) Wood hair removal: a. On the surface of the wooden door, apply a primer layer with a thickness of 0.4mm, a secondary pad...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention discloses a production process for a wooden door, and relates to the field of furniture fitting production methods. The production process includes the steps of board drying, board pressing, cutting, sanding, framing, wood wool removing, paint spraying, drying and package molding. According to the step of wood wool removing, a primer material layer, a secondary slurry layer and an upper-layer polyurethane external photocurable varnish material surface layer with the thicknesses being 0.2-0.4mm are sequentially coated on the surface of the wooden door to serve as a bottom layer, a middle layer and an upper layer of a wooden door surface protective layer in sequence, and then standing lasts for 10-12 minutes; after the upper layer of the protective layer is cured, wood wool exposed out of the surface is swelled and erected, and fiber zymolase is sprayed onto the upper layer and can dissolve the wood wool; and the upper layer is cleaned with clear water and then is dried. By the adoption of the production process for the wooden door, the wood wool can be well removed, and the smoothness of a paint film is improved.

Description

technical field [0001] The invention relates to the field of methods for the production of furniture accessories. Background technique [0002] In wood cutting processing, it is easy to produce many soft fine lignin fibers (wood wool) that have been cut but not completely separated from the wood surface. Although the wood surface has been finely planed, sanded, especially mechanically polished, the finish can be It meets certain requirements, but if you observe carefully, there are still some wood hairs left on the surface of the wood. The formation of wood wool is closely related to the fiber structure and processing conditions of wood. Most woods will produce wood hair, especially elm. Under the action of grinding pressure, these wood hairs often curl up and hide. Once the finishing dye solution, shellac varnish, etc. absorb water or other solvents, they will swell violently and stand upright, resulting in uneven and rough wood surfaces and affecting the paint film. smoo...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): B27M3/18B27M1/08
CPCB27M1/08B27M3/18
Inventor 卢川
Owner CHONGQING KUNXIU DOOR & WINDOW
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products