Industrial wastewater treating agent and preparation method thereof
A technology for industrial wastewater and treatment agent, which is applied in water treatment parameter control, water/sewage treatment, adsorbed water/sewage treatment, etc. The effect of stability, low treatment cost and good adsorption capacity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] An industrial wastewater treatment agent, which is mainly made of the following raw materials in parts by weight: 20 parts of polysilicon aluminum sulfate, 23 parts of iron sulfate, 3 parts of polyacrylamide, 4 parts of microorganisms, 22 parts of cornstarch, chitosan 8 parts, 11 parts of bentonite, 7 parts of zinc sulfate, 8 parts of diatomaceous earth, 30 parts of modified volcanic rock, 15 parts of calcium hydroxide, 15 parts of activated carbon, 9 parts of polyaluminum chloride, 3 parts of menthone and 10 parts of lignin share.
[0024] The preparation method of described modified volcanic stone is as follows:
[0025] (1) pretreatment of the volcanic stone, drying the volcanic stone at a temperature of 90-100°C for 15 hours; then calcining the volcanic stone at a temperature of 550-600°C for 2.5 hours;
[0026] (2) Modification of volcanic stone: after the volcanic stone after step (1) is calcined is cooled, add volcanic stone to 35% hydrochloric acid solution and...
Embodiment 2
[0035] An industrial wastewater treatment agent, which is mainly made of the following raw materials in parts by weight: 15 parts of polysilicon aluminum sulfate, 30 parts of iron sulfate, 1 part of polyacrylamide, 5 parts of microorganisms, 15 parts of corn starch, chitosan 3 parts, 7 parts of bentonite, 10 parts of zinc sulfate, 4 parts of diatomaceous earth, 40 parts of modified volcanic rock, 10 parts of calcium hydroxide, 20 parts of activated carbon, 5 parts of polyaluminum chloride, 1 part of menthone and 5 parts of lignin share.
[0036] The preparation method of described modified volcanic stone is as follows:
[0037] (1) pretreatment of the volcanic stone, drying the volcanic stone at a temperature of 90-100°C for 20 hours; then calcining the volcanic stone at a temperature of 550-600°C for 2 hours;
[0038] (2) Modification of volcanic rock: after the volcanic rock after the calcining in step (1) is cooled, add volcanic rock to 35% hydrochloric acid solution and 2...
Embodiment 3
[0047] An industrial wastewater treatment agent, which is mainly made of the following raw materials in parts by weight: 30 parts of polysilicon aluminum sulfate, 15 parts of ferric sulfate, 5 parts of polyacrylamide, 1 part of microorganism, 30 parts of cornstarch, chitosan 13 parts, 17 parts of bentonite, 5 parts of zinc sulfate, 11 parts of diatomaceous earth, 20 parts of modified volcanic rock, 20 parts of calcium hydroxide, 10 parts of activated carbon, 15 parts of polyaluminum chloride, 5 parts of menthone and 20 parts of lignin share.
[0048] The preparation method of described modified volcanic stone is as follows:
[0049] (1) pretreatment of the volcanic stone, drying the volcanic stone at a temperature of 90-100°C for 10 hours; then calcining the volcanic stone at a temperature of 550-600°C for 3 hours;
[0050] (2) Modification of volcanic stone: after the volcanic stone after step (1) is calcined is cooled, add volcanic stone to 35% hydrochloric acid solution an...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com