A technology of negative ions and silk quilts, applied in the field of bedding, can solve the problems of poor moisture drainage, poor heat preservation effect, and easy to produce bacteria, etc., and achieve the effects of increasing oxygen absorption, improving lung function, and improving UV protection ability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0031] A silk quilt containing negative ions, including core filling, the core filling is made of the following components by weight percentage: 100% pure natural silk 45-50% and anion viscose fiber 50-55%;
[0032] The negative ion viscose fiber contains 0.5-1.5wt% ceramic powder and a coupling agent, and the coupling agent is 0.5-1.5% by weight of the ceramic powder;
[0033] The ceramic powder is made of the following components by weight percentage: zirconia 20-40%, silicon dioxide 20-30%, titanium dioxide 40-50%;
[0034] The coupling agent is made of the following components by weight percentage: 20-30% isopropyl tri(dioctyl phosphate acyloxy) titanate, 20-40% glyceryl stearate, 30-30% glyceryl monostearate 50%.
[0035] Described negative ion viscose fiber is made by following steps:
[0036] (1) Mix zirconium dioxide, silicon dioxide and titanium dioxide, sinter and pulverize them into ceramic powder with an average particle size of 0.2-0.8 μm;
[0037] (2) Mixing a...
Embodiment 2
[0048] A silk quilt containing negative ions, including a core filling, the core filling is made of the following components by weight percentage: 100% pure natural silk 45% and anion viscose fiber 55%;
[0049] Contain 1.0wt% ceramic powder and coupling agent in the negative ion viscose fiber, and coupling agent is 1.0% of ceramic powder weight;
[0050] The ceramic powder is made of the following components by weight: 30% zirconium dioxide, 25% silicon dioxide, and 45% titanium dioxide;
[0051] The coupling agent is made of the following ingredients in weight percent: 25% isopropyl tris(dioctyl phosphate acyloxy) titanate, 25% glyceryl stearate, and 50% glyceryl monostearate.
[0052] Described negative ion viscose fiber is made by following steps:
[0053] (1) Mix zirconium dioxide, silicon dioxide and titanium dioxide, sinter and pulverize them into ceramic powder with an average particle size of 0.2-0.8 μm;
[0054] (2) Mixing a coupling agent with the ceramic powder t...
Embodiment 3
[0066] The same parts of this embodiment and Example 2 will not be repeated, the difference is: the core filling is made of the following components by weight percentage: 100% pure natural silk 46% and negative ion viscose fiber 54% ;
[0067] Contain 0.5wt% ceramic powder and coupling agent in the negative ion viscose fiber, and coupling agent is 1.5% of ceramic powder weight;
[0068] The ceramic powder is made of the following components by weight: 20% zirconium dioxide, 30% silicon dioxide, and 50% titanium dioxide;
[0069] The coupling agent is made of the following ingredients in weight percent: 25% isopropyl tri(dioctyl phosphate acyloxy) titanate, 40% glyceryl stearate, and 35% glyceryl monostearate.
[0070] According to the test of "SFJJ-QWX25-2006 Anion Concentration Inspection Rules", the anion concentration in the product of the present invention is 5240 / cubic centimeter.
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com