A mat, active technology, applied in the direction of manufacturing tools, reed/straw treatment, wood processing appliances, etc., can solve the problems of not having particles, reducing the physical therapy effect, weak field effect, etc., to protect bone growth, relieve discomfort, high field effect, etc. effect of effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0033] 1) Composition by weight of energy powder: 4.3 parts of diamond medicine stone, 4.3 parts of tourmaline, 0.22 parts of Hetian jade, 2.1 parts of coral stone, 3.2 parts of obsidian, 0.05 parts of citrine, 5 parts of medical stone, 3.9 parts of calcium gluconate, 0.5 parts of meteorites, 0.012 parts of zinc glutamate, and 0.25 parts of keel were weighed and mixed thoroughly; then grinded at a temperature of 550 °C with a grinder to obtain energy powder of 2000 mesh to 6000 mesh;
[0034] 2) 26.9 parts of 2000 mesh ~ 6000 mesh energy powder are added with 14% ethanol of the total mass of the energy powder, then transferred to a nano grinder for grinding with a grinding medium of 0.8mm ~ 2.5mm, dried and crushed to obtain nanoscale energy powder ;
[0035] 3) The nano-scale energy powder is weighed according to the mass fraction of 0.18% of the main body of the mat, mixed with the rubber material at a mass ratio of 1:4, and applied to the main body of bamboo mats, bamboo st...
Embodiment 2
[0037] 1) The composition of energy powder by weight is: 4.3 parts of diamond medicine stone, 4.3 parts of tourmaline, 0.22 parts of Hetian jade, 2.3 parts of coral stone, 3.1 parts of obsidian, 0.04 parts of citrine, 4 parts of medical stone, 4.0 parts of calcium gluconate, 0.5 parts of meteorites, 0.014 parts of zinc glutamate, and 0.28 parts of keel were weighed and mixed thoroughly; then grinded with a grinder at a temperature of 545°C to obtain energy powder of 2000 mesh to 6000 mesh;
[0038] 2) 27.0 parts of 2000 mesh ~ 6000 mesh energy powder is added with 14.5% ethanol of the total mass of the energy powder, and then transferred to a nano grinder for grinding with a grinding medium of 0.8 mm ~ 2.5 mm, dried and crushed to obtain nano energy powder ;
[0039] 3) Nano-scale energy powder is weighed according to the mass fraction of 0.20% of the main body of the mat, and then mixed with rubber in a mass ratio of 1:3.9 and applied to the main body of the bamboo mat, bambo...
Embodiment 3
[0041] 1) The composition of energy powder by weight is: 4.1 parts of diamond medicine stone, 4.1 parts of tourmaline, 0.22 parts of Hetian jade, 2.2 parts of coral stone, 3.3 parts of obsidian, 0.05 parts of citrine, 5 parts of medical stone, 3.9 parts of calcium gluconate, 0.5 parts of meteorites, 0.014 parts of zinc glutamate, and 0.23 parts of keels were weighed and mixed thoroughly; then grinded with a grinder at a temperature of 540°C to obtain energy powder of 2000 mesh to 6000 mesh;
[0042] 2) 26.3 parts of 2000 mesh ~ 6000 mesh energy powder are added with 14% ethanol of the total mass of the energy powder, then transferred to a nano grinder for grinding with a grinding medium of 0.8 mm ~ 2.5 mm, dried and crushed to obtain nano energy powder ;
[0043] 3) Nano-scale energy powder is weighed according to the mass fraction of 0.22% of the main body of the mat, mixed with the rubber material at a mass ratio of 1:4.1, and applied to the main body of the bamboo mat, bamb...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com