A drying method, wood drying technology, applied in wood drying, static material dryer, wood humidity control, etc., can solve the problems of not being able to grasp the best drying benchmark of wood, unreasonable data setting, and low drying efficiency, and achieve Promote the use value, shorten the drying time, and promote the effect of water precipitation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0024] A method for drying wood, comprising the steps of:
[0025] (1) Wood pretreatment:
[0026] Cut the wood according to the processing requirements, and then rinse the sawdust and other impurities with clean water before use;
[0027] (2) Pre-drying treatment:
[0028] Put the wood treated in step (1) into the drying room, keep the temperature at 58°C, and the relative air humidity at 50-53%, and dry the wood until the water content is 50-53% for later use;
[0029] (3) Deep drying treatment:
[0030] After the surface of the wood treated in step (2) is coated with a layer of dry powder, it is then placed in an ultrasonic drying chamber for ultrasonic drying of the wood. The relative humidity is 45~48%, just dry the wood until the water content is not more than 10%; the dry powder is made of the following parts by weight: 15 parts of diatomite, 10 parts of bentonite, 6 parts of stearic acid Calcium, 14 parts of silica gel, 5 parts of grafted acrylamide, 6 parts of sod...
Embodiment 2
[0040] A method for drying wood, comprising the steps of:
[0041] (1) Wood pretreatment:
[0042] Cut the wood according to the processing requirements, and then rinse the sawdust and other impurities with clean water before use;
[0043] (2) Pre-drying treatment:
[0044] Put the wood treated in step (1) into the drying room, keep the temperature at 63°C, and the relative air humidity at 53-55%, and dry the wood until the water content is 53-55% for later use;
[0045] (3) Deep drying treatment:
[0046] After the surface of the wood treated in step (2) is coated with a layer of dry powder, it is then placed in an ultrasonic drying chamber for ultrasonic drying of the wood. The relative humidity is 48~50%, just dry the wood until the water content is not more than 10%; the dry powder is made of the following parts by weight: 20 parts of diatomite, 15 parts of bentonite, 8 parts of stearic acid Calcium, 18 parts of silica gel, 7 parts of grafted acrylamide, 10 parts of so...
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com