Method for preparing zinc oxide ore collecting agent
A zinc oxide ore and collector technology, applied in solid separation, flotation, etc., can solve the problems of insignificant effect, impact on buoyancy, and large impact on buoyancy, and achieve less dosage of chemicals and good selection The effect of resistance and low temperature resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] An example of the preparation method of zinc oxide collector of the present invention comprises the following steps:
[0014] First, methyl oleate and methanolamine were mixed in a molar ratio of 1:1 to obtain solution 1, and then sodium hydroxide with a mass percent concentration of 25% was added to solution 1 at a mass ratio of 1:2, and the temperature was 120 Stir at ℃ for 2 hours to prepare solution 2, then add phosphorus pentoxide to solution 2 at 90°C at a mass ratio of 1:1.5 and stir for 3 hours, and finally add sodium hydroxide with a mass percentage concentration of 20% After neutralization, dry at a temperature of 40°C to obtain the zinc oxide ore collector.
Embodiment 2
[0016] Another example of the preparation method of zinc oxide collector of the present invention comprises the following steps:
[0017] First, methyl oleate and methanolamine were mixed at a molar ratio of 2:3 to obtain solution 1, and then sodium hydroxide with a mass percent concentration of 30% was added to solution 1 at a mass ratio of 2:3, at a temperature of 125°C Stir under the same conditions for 2.5 hours to prepare solution 2, then add phosphorus pentoxide to solution 2 at a mass ratio of 1:2 at 90°C and stir for 3.5 hours, and finally add 25% sodium hydroxide to neutralize Then dry at a temperature of 50°C to obtain the zinc oxide ore collector.
Embodiment 3
[0019] This embodiment is an application example of the zinc oxide ore collector in the flotation of zinc oxide ore.
[0020] 1. Mineral raw materials:
[0021] The zinc content in the ore used is 8.24%, the silicon dioxide content is 10.15%, and the iron content is 8.97%. Phase analysis shows that zinc mainly exists in the form of zinc carbonate, and a small amount of zinc silicate and hemimorphite; gangue minerals It mainly exists in the form of silicate, and some limonite and goethite.
[0022] 2. Flotation agents and operating conditions:
[0023] Sodium hexametaphosphate 300g / t
[0024] Water glass rough selection 1000g / t, scanning 300g / t, selection 100g / t
[0025] Salicylaldoxime roughing 200g / t sweeping 100g / t
[0026] The collector roughing 350g / t sweeping 150g / t
[0027] In the flotation process, after the ore is ground until the mineral monomers are dissociated, sodium hexametaphosphate and water glass are added to disperse and inhibit the gangue minerals, then ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com