Kaolin modified mouldproof paper board and preparation method thereof

A kaolin, modified technology, applied in the field of cardboard, can solve the problems of destroying the waterproof effect of the coating layer, reducing the mechanical strength of the carton, and reducing the product quality.

Active Publication Date: 2016-11-09
铜陵锋帆彩色印务股份有限公司
View PDF4 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

Mildew will not only damage the waterproof effect of the paint layer and reduce the mechanical strength of the carton, but also cause a decline in the quality of the products inside the carton.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

preparation example Construction

[0016] The invention provides a method for preparing a kaolin-modified mildew-proof cardboard, comprising:

[0017] 1) The process of decocting Chinese herbal medicines in water to obtain Chinese herbal medicine extracts;

[0018] 2) In the presence of ultraviolet rays, the process of activating kaolin, plant ash, sodium chloroplatinate and molybdenum disulfide to obtain an activated product;

[0019] 3) Under acidic conditions, the process of mixing the activator with the amino acid and performing modification treatment to obtain the modified activator;

[0020] 4) Conduct a contact reaction of acrylic emulsion, polystyrene, dioctyl phthalate, aluminum oxide, boron nitride and sodium nitrite, and then add emulsifiers, modified activators, and Chinese herbal medicine extracts to the reaction system The process of mixing the liquid to make the anti-mildew coating;

[0021] 5) The process of applying the anti-mildew paint to the surface of the cardboard body and drying to obta...

Embodiment 1

[0035] 1) Take mugwort leaf, yam, borneol, honeysuckle vine, Chuanxiong, Tongcao, angelica, kudzu root, Trichosanthes bark, Coptis chinensis, and water according to the ratio of 100:52:48:39:28:77:42:31:36:92:500 Mixed by weight, and decocted at 160°C for 5 hours to obtain Chinese herbal medicine extract;

[0036] 2) In the presence of ultraviolet rays with a wavelength of 230nm, kaolin, plant ash, sodium chloroplatinate and molybdenum disulfide were mixed in a weight ratio of 100:62:19:37, and activated at 80°C for 14 hours to obtain an activated product;

[0037] 3) Under the condition of pH 5, the activated substance was mixed with amino acid (weight ratio 100:55) and modified at 55°C for 8 hours to obtain the modified activated substance;

[0038] 4) Mix acrylic emulsion, polystyrene (weight-average molecular weight: 5000), dioctyl phthalate, aluminum oxide, boron nitride and sodium nitrite, and mix them at 100°C and a vacuum of 8MPa The contact reaction was carried out f...

Embodiment 2

[0042] 1) Take mugwort leaf, yam, borneol, honeysuckle vine, Chuanxiong, Tongcao, angelica, kudzu root, Trichosanthes bark, Coptis chinensis, and water according to the ratio of 100:45:42:36:24:74:36:22:29:88:400 Mixed in weight ratio, and decocted at 150°C for 4 hours to obtain Chinese herbal medicine extract;

[0043] 2) In the presence of ultraviolet light with a wavelength of 200nm, kaolin, plant ash, sodium chloroplatinate and molybdenum disulfide were mixed in a weight ratio of 100:55:14:32, and activated at 75°C for 12 hours to obtain an activated product;

[0044] 3) Under the condition of pH 4, the activated substance was mixed with amino acid (weight ratio 100:47) and then modified at 50°C for 6 hours to obtain the modified activated substance;

[0045] 4) Mix acrylic emulsion, polystyrene (weight-average molecular weight: 3000), dioctyl phthalate, aluminum oxide, boron nitride and sodium nitrite, and mix them at 95°C and a vacuum of 5MPa The contact reaction was carr...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

PropertyMeasurementUnit
wavelengthaaaaaaaaaa
Login to view more

Abstract

The invention discloses a kaolin modified mouldproof paper board and a preparation method thereof. The preparation method comprises the following steps: 1) putting Chinese herbal medicines into water to be decocted, so as to obtain a Chinese herbal medicine extracting solution; 2) in presence of ultraviolet ray, carrying out activating treatment on kaolin, plant ash, sodium chloroplatinate and molybdenum disulfide, so as to obtain an activator; 3) under acidic condition, mixing the activator with amino acid, and then modifying, so as to obtain a modified activator; 4) carrying out contact reaction on acrylic emulsion, polystyrene, dioctyl phthalate, aluminium oxide, boron nitride and sodium nitrite, then adding an emulsifying agent, the modified activator and the Chinese herbal medicine extracting solution, and mixing, so as to obtain mouldproof paint; and 5) coating the mouldproof paint on the surface of a paper board body, and drying, so that the kaolin modified mouldproof paper board is obtained. The mouldproof paper board has excellent mechanical, waterproof and antibacterial properties.

Description

technical field [0001] The invention relates to a cardboard, in particular to a kaolin-modified mildew-resistant cardboard and a preparation method thereof. Background technique [0002] Carton is currently the most common form of outer packaging for most products, and it is the first line of defense to protect product appearance, function, integrity, etc., and because water is the biggest culprit that causes damage to the appearance and function of many products, consumers are very concerned about cartons. Water resistance has extremely high requirements. [0003] The method of enhancing the waterproofness of cartons is mainly to add a waterproof coating layer on the surface of the carton, and the method of adding coating is mainly organic printing, manual brushing, spraying, etc. Existing waterproof coatings for cartons generally contain a large amount of macromolecules. After the cartons are used for a long time, the coating layer on the surface of the cartons will becom...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): D21H21/16D21H21/36D21H19/10
CPCD21H19/10D21H21/16D21H21/36
Inventor 解和锋沐磊
Owner 铜陵锋帆彩色印务股份有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products