Method for innocent treatment of arsenic sulfide residues
A technology of harmless treatment and arsenic sulfide, which is applied in the direction of protection devices against harmful chemicals, can solve the problems of long stirring time and high energy consumption, and achieve the effects of short stirring time, low energy consumption and simple process flow
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] At room temperature, weigh 100g of arsenic sulfide slag, add 50mL of water, add sodium sulfide (Na 2 S), stirred and reacted until the pH value was 9, placed in a reactor and stirred evenly, and reacted for 60 minutes; added 5 mL of hydrogen peroxide, and oxidized for 30 minutes; added 6 g of polyferric sulfate (PFS), stirred for 20 minutes to complete the stabilization of arsenic; , stirring for 5 minutes; maintenance.
[0022] Performance test: According to the solid waste toxic leaching method-horizontal oscillation method (GB 5086.2-1997), the arsenic leaching concentration meets the pollution control standard of hazardous waste landfill (GB 18598-2001).
Embodiment 2
[0024] At room temperature, weigh 100g of arsenic sulfide slag, add 50mL of water, add sodium sulfide (Na2S), stir the reaction until the pH value is 10, put it in the reactor and stir evenly, and react for 40min; add 5mL of hydrogen peroxide, oxidize for 30min; add 5g Add ferrous sulfate, stir for 20 minutes to complete the stabilization of arsenic; add 20g of cement, stir for 5 minutes; carry out curing.
[0025] Performance test: According to the solid waste toxic leaching method-horizontal oscillation method (GB 5086.2-1997), the arsenic leaching concentration meets the pollution control standard of hazardous waste landfill (GB 18598-2001).
Embodiment 3
[0027] At room temperature, weigh 100g of arsenic sulfide slag, add 50mL of water, add sodium sulfide (Na2S), stir the reaction until the pH value is 11, put it in the reactor and stir evenly, react for 30min; add 5mL of hydrogen peroxide, oxidize for 30min; add 6g Add polyaluminum chloride (PAC) and stir for 20 minutes to complete the stabilization of arsenic; add 20g of cement and stir for 5 minutes; perform curing.
[0028] Performance test: According to the solid waste toxic leaching method-horizontal oscillation method (GB 5086.2-1997), the arsenic leaching concentration meets the pollution control standard of hazardous waste landfill (GB 18598-2001).
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com