A technology of sludge and bamboo charcoal, which is applied in biological sludge treatment, chemical instruments and methods, water/sludge/sewage treatment, etc., can solve the problems of huge capital investment, and achieve cost reduction, high compressive strength, and thermal conductivity The effect of a small coefficient
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] A method of using sludge is to deodorize the sludge and mix it with bamboo charcoal, sepiolite, foaming agent, potassium feldspar, expanded perlite, calcined kaolin, wollastonite powder, sodium lauryl sulfate Together to make insulation bricks. Among them, the parts by weight of each material are: 80 parts of sludge, 11 parts of bamboo charcoal, 10 parts of sepiolite, 15 parts of foaming agent, 21 parts of potassium feldspar, 8 parts of expanded perlite, 7.5 parts of calcined kaolin, wollastonite powder 4.5 parts, 3 parts of sodium lauryl sulfate.
[0016] The process of the deodorization treatment is: according to the ratio of adding 80 grams of deodorant per ton of sludge, mix and place for 8 days; the deodorant is loaded with denitrification microbial flora and EM flora mixed bacteria Microbial carrier; the microbial carrier is mixed with vermiculite, sawdust and clay according to the weight ratio of 1:4:0.25, and then pressed into granular form after adding binder....
Embodiment 2
[0019] A method of using sludge is to deodorize the sludge and mix it with bamboo charcoal, sepiolite, foaming agent, potassium feldspar, expanded perlite, calcined kaolin, wollastonite powder, sodium lauryl sulfate Together to make insulation bricks. Among them, the parts by weight of each material are: 50 parts of sludge, 15 parts of bamboo charcoal, 5 parts of sepiolite, 18 parts of foaming agent, 15 parts of potassium feldspar, 10 parts of expanded perlite, 5 parts of calcined kaolin, wollastonite powder 10 parts, 1 part of sodium lauryl sulfate.
[0020] The process of the deodorization treatment is: according to the ratio of adding 100 grams of deodorant per ton of sludge, mix and place for 5 days; the deodorant is loaded with denitrification microbial flora and EM flora mixed bacteria Microbial carrier; the microbial carrier is mixed with vermiculite, sawdust and clay according to the weight ratio of 1:5:0.1, and then pressed into granular form after adding binder.
...
Embodiment 3
[0023] A method of using sludge is to deodorize the sludge and mix it with bamboo charcoal, sepiolite, foaming agent, potassium feldspar, expanded perlite, calcined kaolin, wollastonite powder, sodium lauryl sulfate Together to make insulation bricks. Among them, the parts by weight of each material are: 100 parts of sludge, 5 parts of bamboo charcoal, 15 parts of sepiolite, 10 parts of foaming agent, 25 parts of potassium feldspar, 5 parts of expanded perlite, 10 parts of calcined kaolin, wollastonite powder 1 part, 5 parts of sodium lauryl sulfate.
[0024] The process of the deodorization treatment is: according to the ratio of adding 50 grams of deodorant per ton of sludge, mix and place for 10 days; the deodorant is loaded with denitrification microbial flora and EM flora mixed bacteria Microbial carrier; the microbial carrier is mixed with vermiculite, sawdust and clay according to the weight ratio of 1:2:0.5, and then pressed into granular form after adding binder.
...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com