Welding electrode coating and method of preparing same into welding electrode

A welding rod coating and coating technology, which is applied in welding equipment, manufacturing tools, welding media, etc., can solve the problems of difficult machining of welded joints, fast cooling speed, and easy cracking, and achieves good machining performance and arc combustion. Stable, smooth seam formation

Active Publication Date: 2016-07-27
HENAN POLYTECHNIC
View PDF10 Cites 5 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

Due to the extremely poor weldability of gray cast iron, there are mainly the following problems in welding repair: First, the welded joint is difficult to machine. Easy to produce cementite (Fe 3 C) White structure is formed, and the hardness of white cast iron structure is as high as HB800, which makes it difficult to machine gray iron parts after welding repair
The second is that the welded joints are prone to cracks. Gray cast iron itself has low strength and poor plasticity, and the uneven heating during the welding process causes cracks to easily occur in the weld seam and heat-affected zone. Much larger, making the stress more severe and increasing the tendency to crack
[0004] At present, there are many types of welding electrodes specially used for gray cast iron welding repair, but there are very few welding electrodes that can meet the weldability requirements of gray cast iron and reduce welding costs

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0019] An electrode coating, in parts by weight, the electrode coating is composed of the following powder components: 5 parts of rutile, 22 parts of reduced ilmenite, 6 parts of kaolin, 15 parts of light calcium powder, 24 parts of iron red, talcum powder 4 parts, 10 parts of aluminum powder, 3 parts of alkali flour, 4 parts of wood powder, 4 parts of titanium dioxide, 3 parts of ferromanganese; the binder of electrode coating is sodium silicate water glass, and every 100g of electrode coating powder Add 30g of water glass.

[0020] According to the above weight ratio, weigh the above powder and mix it evenly in the mixing machine to obtain a mixed powder. Add a binder to the mixed powder and then press-coat it on the welding core. The weight coefficient of the coating is 0.3, and then put it in the oven After drying, the welding rod of this embodiment is obtained.

Embodiment 2

[0022] An electrode coating, in parts by weight, the electrode coating is composed of the following powder components: 7 parts of rutile, 18 parts of reduced ilmenite, 6 parts of kaolin, 16 parts of light calcium powder, 22 parts of iron red, talcum powder 4 parts, 10 parts of aluminum powder, 3 parts of alkali flour, 5 parts of wood powder, 4 parts of titanium dioxide, 5 parts of ferromanganese; Add 36g of water glass.

[0023] According to the above weight ratio, weigh the above powder and mix it evenly in the mixing machine to obtain a mixed powder. Add a binder to the mixed powder and then press-coat it on the welding core. The weight coefficient of the coating is 0.3, and then put it in the oven After drying, the welding rod of this embodiment is obtained.

Embodiment 3

[0025] An electrode coating, in parts by weight, the electrode coating is composed of the following powder components: 5 parts of rutile, 20 parts of reduced ilmenite, 6 parts of kaolin, 13 parts of light calcium powder, 24 parts of iron red, 4 parts of talcum powder 12 parts of aluminum powder, 2 parts of alkali flour, 5 parts of wood powder, 4 parts of titanium dioxide, and 5 parts of ferromanganese; the binder of the electrode coating is potassium silicate water glass, and 30g water glass.

[0026] According to the above weight ratio, weigh the above powder and mix it evenly in the mixing machine to obtain a mixed powder. Add a binder to the mixed powder and then press-coat it on the welding core. The weight coefficient of the coating is 0.45, and then put it in the oven After drying, the welding rod of this embodiment is obtained.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
tensile strengthaaaaaaaaaa
hardnessaaaaaaaaaa
Login to View More

Abstract

The invention discloses a welding electrode coating. The welding electrode coating is composed of, by weight, 5-7 parts of diamond, 18-22 parts of reduced ilmenite, 4-6 parts of kaolin, 13-16 parts of light calcium powder, 22-25 parts of iron red, 2-4 parts of talcum powder, 10-14 parts of aluminum powder, 1-3 parts of sodium carbonate, 4-6 parts of wood meal, 4-7 parts of titanium dioxide and 3-6 parts of ferromanganese. A binder of the welding electrode coating is sodium silicate or potassium silicate water glass, and 30-36 g of water glass is added into each100 g of the welding electrode coating. Raw materials are low in price, so that the coating prepared is low in cost. When the welding electrode prepared by the welding electrode coating is used for welding, welding defects like air holes, slag inclusion and cracks do not appear on the welding surface, and welding seam forming is smooth; an electric arc is stable in burning, splashing particles are small, slag removing is easy after welding, and the coating is uniform in melting and free of caking and shedding; a conventional knife and conventional cutting parameters are adopted to machine a welding joint, knife beating in the machining process is avoided, no knife relieving trace is formed on a cut surface, and machining performance is good.

Description

technical field [0001] The invention belongs to the field of welding materials, and in particular relates to a welding rod coating and a method for preparing it into a welding rod. Background technique [0002] As an important engineering material, cast iron is widely used in the machinery manufacturing industry due to its low cost, good casting performance, and excellent shock absorption performance. Among them, gray cast iron is the most widely used cast iron, and its output accounts for more than 80% of the total output of cast iron. Among the blanks of mechanical equipment, gray iron parts account for about 50%. According to statistics, in the production of castings, the scrap rate is as high as 20% due to various reasons, and the loss is serious. [0003] At present, the best way to reduce losses is to repair the waste products through repair welding. Due to the extremely poor weldability of gray cast iron, there are mainly the following problems in welding repair: Fi...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): B23K35/365B23K35/40
CPCB23K35/365B23K35/404
Inventor 李晓东邓小君任艳艳蒋智霞刘文娟王小林冯金广孙宇瀚解鹏程金宁宁袁鹏孙雅倩
Owner HENAN POLYTECHNIC
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products