Solid-waste recycling treating method
A treatment method and resource recovery technology, applied in the field of solid waste resource recovery, can solve problems such as hindering soil capillary water and natural water penetration, groundwater difficult to secondary salinization of soil, hindering crop growth and development, etc., to improve mechanical properties and flame retardant performance, low cost, low cost effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0032] Prepare waste circuit board resin powder with a mass fraction of 80%, waste agricultural film powder with a mass fraction of 10% in a particle size range of 5 to 10mm, and desulfurized gypsum powder with a mass percentage of 10% in a particle size range of 1 to 5mm. Fully mix in the blender, add zinc stearate accounting for 0.1% of the weight of the mixture, add EVA latex accounting for 0.5% of the weight of the mixture, add sodium dodecylsulfonate accounting for 0.1% of the weight of the mixture, add 0.1% of the weight of the mixture 0.1% magnesium-aluminum hydrotalcite, stir and mix evenly; fully mix the treated mixed material with cement powder according to the mass percentage of 85%, add 0.1% active alumina by weight of the mixed material, and then add appropriate amount of water for stirring Mix to form a slurry; inject the slurry into the test mold and cast it into shape; place the test mold injected with the slurry on a vibrator to vibrate for 5 minutes to remove ...
Embodiment 2
[0034] Prepare waste circuit board resin powder with a mass fraction of 60%, waste agricultural film powder with a mass fraction of 20% in a particle size range of 5 to 10mm, and desulfurized gypsum powder with a mass percentage of 20% in a particle size range of 1 to 5mm. Fully mix in the blender, add zinc stearate accounting for 0.5% of the weight of the mixture, add EVA latex accounting for 0.1% of the weight of the mixture, add sodium dodecylsulfonate accounting for 0.5% of the weight of the mixture, add 0.5% of the weight of the mixture 0.5% magnesium-aluminum hydrotalcite, stir and mix evenly; fully mix the treated mixture with cement powder according to 100% by mass, add activated alumina accounting for 1% of the weight of the mixture, and then add appropriate amount of water for stirring Mix to form a slurry; inject the slurry into the test mold and cast it into shape; place the test mold injected with the slurry on a vibrator to vibrate for 5 minutes to remove air bubb...
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
particle size | aaaaa | aaaaa |
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com