A post-finishing and environment-friendly technology, applied in leather surface treatment, small raw hide/big raw hide/leather/fur treatment, small raw hide/large raw hide/leather skin/fur chemical treatment, etc., can solve single function, affect production, Environmental pollution and other problems, to achieve the effect of improving brightness, improving environmental protection performance, and improving overall performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0055] The composition of each raw material in the environment-friendly antibacterial fur finishing agent of the present embodiment is as follows according to weight percentage:
[0056]
[0057] A preparation method of an environment-friendly antibacterial fur finishing agent, comprising the steps of:
[0058] (1) Put fatty alcohol, organosilicon, and nonionic surfactant into the reactor, and heat to 50-60 degrees, and stir evenly after dissolving;
[0059] (2) Properly dissolve the quaternary ammonium salt with 20% deionized water, and set aside;
[0060] (3) Slowly add the remaining deionized water into the reactor, after mixing evenly, start to cool down;
[0061] (4) Cool the material to 10-15 degrees, add quaternary ammonium salt solution and preservative, and stir well to obtain an environment-friendly antibacterial fur finishing agent.
Embodiment 2
[0063] The composition of each raw material in the environment-friendly antibacterial fur finishing agent of the present embodiment is as follows according to weight percentage:
[0064]
[0065] A preparation method of an environment-friendly antibacterial fur finishing agent, comprising the steps of:
[0066] (1) Put fatty alcohol, organosilicon, and nonionic surfactant into the reactor, and heat to 80-90 degrees, and stir evenly after dissolving;
[0067] (2) Properly dissolve the quaternary ammonium salt with 50% deionized water, and set aside;
[0068] (3) Slowly add the remaining deionized water into the reactor, after mixing evenly, start to cool down;
[0069] (4) Cool the material to 25-30 degrees, add a quaternary ammonium salt solution and a preservative, and stir evenly to obtain an environment-friendly antibacterial fur finishing agent.
Embodiment 3
[0071] The composition of each raw material in the environment-friendly antibacterial fur finishing agent of the present embodiment is as follows according to weight percentage:
[0072]
[0073] A preparation method of an environment-friendly antibacterial fur finishing agent, comprising the steps of:
[0074] (1) Put fatty alcohol, organosilicon, and nonionic surfactant into the reactor, and heat to 50-60 degrees, and stir evenly after dissolving;
[0075] (2) Properly dissolve the quaternary ammonium salt with 25% deionized water, and set aside;
[0076] (3) Slowly add the remaining deionized water into the reactor, after mixing evenly, start to cool down;
[0077] (4) Cool the material to 15-20 degrees, add quaternary ammonium salt solution and preservative, and stir well to obtain an environment-friendly antibacterial fur finishing agent.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com