Novel light waterproof building material and preparation method thereof
A waterproof building material and building material technology, applied in the field of new lightweight waterproof building materials and their preparation, can solve the problems of incomplete bonding, poor environmental protection performance, and joints, so as to reduce the load of buildings, achieve good sound insulation effects, The effect of weight reduction
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] A new type of lightweight waterproof building material, characterized in that the building material is composed of the following components in parts by weight: 6 parts of diatomite, 35 parts of acrylate, 5 parts of phenolic resin, 100 parts of magnesium oxide, heavy carbonic acid 10 parts of calcium, 9 parts of plant fiber, 4 parts of kaolin, 3 parts of gypsum powder, 4 parts of quartz sand, 5 parts of pine sawdust, 6 parts of natural shale powder, 1 part of saponification agent, 0.2 parts of wetting agent, film-forming aid 1.5 parts, 0.5 parts of stabilizer, 0.6 parts of waterproofing agent, 0.2 parts of fungicide, 10 parts of glass fiber and 50 parts of water.
[0020] Further, the stabilizer is barium stearate.
[0021] The preparation method of the novel lightweight waterproof building material composed of the above components comprises the following steps:
[0022] (1) Add 6 parts of diatomaceous earth, 35 parts of acrylate, 5 parts of phenolic resin, 100 parts of...
Embodiment 2
[0029] A new type of lightweight waterproof building material, which is composed of the following components in parts by weight: 7 parts of diatomite, 40 parts of acrylate, 10 parts of phenolic resin, 120 parts of magnesium oxide, 15 parts of heavy calcium carbonate, and 11 parts of plant fiber 6 parts of kaolin, 3.5 parts of gypsum powder, 5 parts of quartz sand, 6 parts of pine sawdust, 8.5 parts of natural shale powder, 6 parts of saponification agent, 0.3 parts of wetting agent, 2 parts of film-forming aid, 1.5 parts of stabilizer , 0.7 parts of waterproofing agent, 0.25 parts of fungicide, 13 parts of glass fiber and 65 parts of water.
[0030] Further, the stabilizer is barium stearate.
[0031] The preparation method of the novel lightweight waterproof building material composed of the above-mentioned components is prepared by the method in Example (1).
Embodiment 3
[0033] A new type of lightweight waterproof building material, which is composed of the following parts by weight: 9 parts of diatomite, 45 parts of acrylate, 15 parts of phenolic resin, 150 parts of magnesium oxide, 20 parts of heavy calcium carbonate, and 12 parts of plant fiber 7 parts of kaolin, 4 parts of gypsum powder, 6 parts of quartz sand, 7 parts of pine sawdust, 10 parts of natural shale powder, 9 parts of saponifier, 0.4 part of wetting agent, 2.5 parts of film-forming aid, 2.5 parts of stabilizer , 0.8 parts of waterproofing agent, 0.3 parts of antifungal agent, 15 parts of glass fiber and 70 parts of water.
[0034] Further, the stabilizer is barium stearate.
[0035] The preparation method of the novel lightweight waterproof building material composed of the above-mentioned components is prepared by the method in Example (1).
PUM
![No PUM](https://static-eureka-patsnap-com.libproxy1.nus.edu.sg/ssr/23.2.0/_nuxt/noPUMSmall.5c5f49c7.png)
Abstract
Description
Claims
Application Information
![application no application](https://static-eureka-patsnap-com.libproxy1.nus.edu.sg/ssr/23.2.0/_nuxt/application.06fe782c.png)
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com