[0058] An environment-friendly sewage treatment agent, according to parts by weight, the composition ratio is as follows: 40 parts of coconut shell charcoal, 70 parts of bamboo charcoal, 15 parts of opal shale, 12 parts of zeolite, 8 parts of montmorillonite, 10 parts of brucite, poly 20 parts of ferric silicosulfate, 30 parts of polyaluminum ferric acid.
[0059] Its preparation method, concrete steps are:
[0060] (1) Grinding bamboo charcoal, opal shale, polysilicate ferric sulfate, and polyaluminum iron bis-acid to 200 mesh, and mixing them uniformly to obtain the first mixed product;
[0061] (2) Crush the montmorillonite to 200 mesh, add it to ammonia water with a mass concentration of 5%, and impregnate it at room temperature for 24 hours, wash and filter it with deionized water, and then dry it in vacuum for 12 hours at a temperature lower than 363K;
[0062] (3) Wash the natural zeolite with deionized water for 6-8 times to remove the inorganic impurities on the surf...
Embodiment 2
[0066] An environment-friendly sewage treatment agent, according to parts by weight, the composition ratio is as follows: 50 parts of coconut shell charcoal, 60 parts of bamboo charcoal, 16 parts of opal shale, 11 parts of zeolite, 9 parts of montmorillonite, 12 parts of brucite, poly 12 parts of ferric silicosulfate, 35 parts of polyaluminum ferric acid.
[0067] (1) Grinding bamboo charcoal, opal shale, zeolite, polysilicoferric sulfate, and polyaluminum iron bis-acid to 200 mesh, and mixing them uniformly to obtain the first mixed product;
[0068] (2) Crush the montmorillonite to 325 mesh, add it to ammonia water with a mass concentration of 10%, impregnate it at room temperature for 24 hours, wash and filter it with deionized water, and then dry it in vacuum, and dry it at a temperature lower than 363K for 12 hours;
[0069] (3) Wash the natural zeolite with deionized water for 6-8 times to remove the inorganic impurities on the surface, then impregnate it with a HClO sol...
Embodiment 3
[0073] An environment-friendly sewage treatment agent, according to parts by weight, the composition ratio is as follows: 60 parts of coconut shell charcoal, 50 parts of bamboo charcoal, 17 parts of opal shale, 10 parts of zeolite, 10 parts of montmorillonite, 14 parts of brucite, poly 16 parts of ferric silicosulfate, 30 parts of polyaluminum ferric acid.
[0074] (1) Grinding bamboo charcoal, opal shale, zeolite, polysilicoferric sulfate, and polyaluminum iron bis-acid to 325 mesh, and mixing them uniformly to obtain the first mixed product;
[0075] (2) Crush the montmorillonite to 400 mesh, add it to ammonia water with a mass concentration of 15%, impregnate it at room temperature for 24 hours, wash and filter it with deionized water, and then dry it in vacuum, and dry it at a temperature lower than 363K for 12 hours;
[0076] (3) Wash the natural zeolite with deionized water for 6-8 times to remove the inorganic impurities on the surface, take out the zeolite and put it i...
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com