An adhesive, environmentally friendly technology, applied in the direction of adhesive types, cellulose adhesives, conjugated diene adhesives, etc., can solve the problems of polluting the environment, affecting human health, etc. The preparation method is simple and easy to implement, and the bonding effect is good.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] The prescription of present embodiment is as follows:
[0024] SBR 5%;
[0025] Glycerin fatty acid ester 2%;
[0028] Polyethylene glycol 10%;
[0029] The balance is water.
[0030] The preparation method of this embodiment is as follows:
[0031] 1. According to the composition ratio of the ingredients, weigh the glycerin fatty acid ester required for the formula, and add it to the preparation container.
[0032] 2. Add the styrene-butadiene rubber required by the formula into the preparation container in turn, and stir with a mixer for 10 minutes after each substance is added, so that it can be fully emulsified with the emulsifier.
[0033] 3. Following step 2, sequentially add sodium aluminate, sodium aluminate and polyethylene glycol required by the formula into the preparation container. Stir with a mixer for 10 minutes to fully dissolve it.
[0034] 4. Following step 3, add water to 100% in the p...
Embodiment 2
[0036] The prescription of present embodiment is as follows:
[0037] Polyurethane 10%;
[0038] Sucrose fatty acid ester 5%;
[0040] Sodium aluminate 5%;
[0041] Isopropanol 30%;
[0042] The balance is water.
[0043] The preparation method of this embodiment is as follows:
[0044] 1. According to the composition ratio of the ingredients, weigh the sucrose fatty acid ester required for the formula, and add it to the preparation container.
[0045] 2. Add the polyurethane required by the formula into the preparation container in turn, and stir with a mixer for 20 minutes after each substance is added, so that it can be fully emulsified with the emulsifier.
[0046] 3. Following step 2, add sodium aluminate, sodium aluminate and isopropanol required for the formula into the preparation container in sequence. Stir with a mixer for 20 minutes to fully dissolve it.
[0047] 4. Following step 3, add water to 100% in the preparation container...
Embodiment 3
[0049] The prescription of present embodiment is as follows:
[0050] Nitrocellulose 20%;
[0051] Sorbitan fatty acid ester + propylene glycol fatty acid ester 10%, sorbitan fatty acid ester: propylene glycol fatty acid ester = 5:5 (weight ratio);
[0052] Sodium silicate 10%;
[0053] Sodium aluminate 10%;
[0054] Ethyl acetate 30%;
[0055] The balance is water.
[0056] The preparation method of this embodiment is as follows:
[0057] 1. According to the proportion of ingredients, weigh the sorbitan fatty acid ester and propylene glycol fatty acid ester required for the formula, and add them to the preparation container.
[0058] 2. Add the nitrocellulose required by the formula into the preparation container in turn, and stir with a mixer for 30 minutes after each substance is added to make it fully emulsified with the emulsifier.
[0059] 3. Following step 2, sequentially add sodium aluminate, sodium aluminate and ethyl acetate required for the formula into the pr...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology