Independent silver ore flotation method
A silver ore, independent technology, applied in the flotation field of independent silver ore, can solve the problems of low recovery rate, serious package, many types, etc., to achieve the effect of improving grade and recovery rate, reducing metallurgical cost, and improving utilization efficiency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] Put the independent silver ore containing 140g / t of silver into the mill, and grind the ore (through wet grinding) until 80% of the silver minerals in it are dissociated; put the ore slurry after grinding into the flotation tank, add lead The galena concentrate with a content of 50% (the amount of lead ore concentrate added is 3% of the mass of independent silver ore) is fully stirred, and 2000g / t of sodium sulfide is added to sulfide the silver oxide minerals, and 50g / t is added The butyl xanthate and 200g / t butyl ammonium black powder are used as collectors for silver minerals. After three times of roughing, one sweeping and three times of beneficiation, the silver concentrate product is obtained.
[0022] The grade of silver in the obtained concentrate is 5150g / t, and the recovery rate is 71%; the grade of lead is 48%, and the recovery rate is 62%.
Embodiment 2
[0024] Put the independent silver ore containing 100g / t of silver into the mill, and grind until 85% of the silver ore in it is dissociated. Put the ore pulp after grinding into the flotation tank, add white lead ore concentrate with a lead content of 65% (the amount of lead ore concentrate is 1% of the mass of independent silver ore) and stir well, add 1500g / t of Sodium sulfide, sulfide the silver oxide minerals in it, add 150g / t butyl xanthate and 150g / t butyl ammonium black powder as collectors for silver minerals, after three times of roughing, one time of sweeping, three times of beneficiation, Obtain silver concentrate product.
[0025] The grade of silver in the obtained concentrate is 5900g / t, and the recovery rate is 67%; the grade of lead is 42%, and the recovery rate is 73%.
Embodiment 3
[0027] Put the independent silver ore containing 170g / t of silver into the mill, and grind until 90% of the silver ore in it is dissociated. Put the ore pulp after grinding into the flotation tank, add lead ore concentrate with a lead content of 58% (the amount of lead ore concentrate added is 4% of the mass of independent silver ore) and fully stir, wherein, the lead ore concentrate Chinese galena accounts for 70%, white lead ore accounts for 30%, adding 500g / t of sodium sulfide to sulfide the silver oxide minerals, adding 200g / t of butyl xanthate and 50g / t of butylammonium black medicine, as silver Mineral collector, after three times of roughing, one time of sweeping and three times of beneficiation, the silver concentrate product is obtained.
[0028] The grade of silver in the obtained concentrate is 4860g / t, and the recovery rate is 75%; the grade of lead is 54%, and the recovery rate is 61%.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com