A kind of multi-dimensional element dispersible tablet
A technology of multi-dimensional elements and dispersible tablets, which is applied in the direction of inorganic active ingredients, organic active ingredients, iodine compound active ingredients, etc. It can solve the problems of multi-dimensional element tablets with many main ingredients, unstable main drugs, and great difficulty, and achieve fast disintegration , Coordinating the effects of enhancing immunity and improving product quality
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0033] Select the WP50N / 75 roller press manufactured by Alexander Company in Germany;
[0034] The water-soluble chitosan in this example is purchased from Guangzhou Shengtong Trading Co., Ltd., or can be prepared by itself according to the existing technology. The molecular weight of the chitosan is 1300-1600.
[0035] A preparation method of multidimensional element dispersible tablet:
[0036] The following raw materials were prepared into 1000 pieces;
[0037]
[0038]
[0039]Preparation of granules: Divide the above raw materials into A, B, and C materials, pre-mix A, B, and C materials respectively, and then use a dry granulation machine to obtain granules, then add magnesium stearate to the A, B, and C granules, and polymerize Povidone K30 6g and crospovidone are mixed evenly and granulated;
[0040] The A material is: vitamin A acetate powder, vitamin E powder, vitamin D3, vitamin B2, vitamin B12, vitamin B1, vitamin B6, magnesium oxide, potassium sulfate, man...
Embodiment 2
[0047] Select the WP50N / 75 roller press manufactured by Alexander Company in Germany;
[0048] The water-soluble chitosan in this example is purchased from Guangzhou Shengtong Trading Co., Ltd., or can be prepared by itself according to the existing technology. The molecular weight of the chitosan is 1300-1600.
[0049] A preparation method of multidimensional element dispersible tablet:
[0050] The following raw materials were prepared into 1000 pieces;
[0051]
[0052]
[0053]
[0054] Preparation of granules: Divide the above raw materials into A, B, and C materials, pre-mix A, B, and C materials respectively, and then use a dry granulation machine to obtain granules, then add magnesium stearate to the A, B, and C granules, and polymerize Mix 7.25g of vitamin K30 and crospovidone evenly to make granules;
[0055] The A material is: vitamin A acetate powder, vitamin E powder, vitamin D3, vitamin B2, vitamin B12, vitamin B1, vitamin B6, magnesium oxide, potassiu...
Embodiment 3
[0062] Select the WP50N / 75 roller press manufactured by Alexander Company in Germany;
[0063] The water-soluble chitosan in this example is purchased from Guangzhou Shengtong Trading Co., Ltd., or can be prepared by itself according to the existing technology. The molecular weight of the chitosan is 1300-1600.
[0064] A preparation method of multidimensional element dispersible tablet:
[0065] The following raw materials were prepared into 1000 pieces;
[0066]
[0067]
[0068] Preparation of granules: Divide the above raw materials into A, B, and C materials, pre-mix A, B, and C materials respectively, and then use a dry granulation machine to obtain granules, then add magnesium stearate to the A, B, and C granules, and polymerize Povidone K30 5g and crospovidone were mixed evenly and granulated;
[0069] The A material is: vitamin A acetate powder, vitamin E powder, vitamin D3, vitamin B2, vitamin B12, vitamin B1, vitamin B6, magnesium oxide, potassium sulfate, m...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com